Fachartikel in der Zeitschrift Waste Management, 2023-06. Verfasst von Hailong Li und 4 weiteren Autor:innen. Beteiligte Einrichtung: School of Energy Science and Engineering, Central South University, Changsha 410083, China. Hauptthemen laut MEDLINE: Incineration, Sewage. Die Arbeit wurde bisher 20-mal zitiert (Crossref) und nennt 43 Literaturangaben. Gefördert von: National Natural Science Foundation of China National Outstanding Youth Science Fund Project, National Natural Science Foundation of China, Natural Science Foundation of Hunan Province.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Rotary kiln incineration is a desirable disposal option for steel-rolling oily sludge. However, ringing remains a key challenge in the highly efficient operation of rotary kilns. This study investigates the erosion behaviour of refractory bricks in a rotary kiln during steel-rolling oily sludge incineration and its effects on ringing. The degree of refractory brick erosion (i.e. iron permeation-depth and quantity) depends on the roasting temperature and time. The iron permeation-depth (3.1 mm) after 36 h of roasting at 1350 °C is greater than that (0.7 mm) after 12 h of roasting at 1200 °C. In the same zones of the refractory bricks, iron permeation increases with the roasting temperature and time. This is because the molten substances generated from the steel-rolling oily sludge erode the refractory bricks, whereas the loosened surface of the eroded refractory bricks is conducive to the continual permeation of molten substances in the refractory bricks. Steel-rolling oily sludge is mixed with refractory brick powder to produce briquettes, which are then used to simulate the permeation and erosion processes. Adding 20% refractory bricks to the briquettes decreases the cohesion strength of the briquettes from 9.07 to 11.71 kN to 2.97-4.44 kN when roasting is performed at 1250 °C for 5-30 min. Although haematite contributes to the high cohesive strength of the rings, the primary components of the refractory brick are transformed into eutectic substances, which decreases the cohesive strength of the rings. These findings provide a useful reference for developing ringing mitigation methods for rotary kilns.

Schlagwörter

MeSH-Schlagwörter (MEDLINE)

IncinerationSewageSteelIronOils

Stichwörter der Autor:innen

Refractory brickRingingRotary kilnSteel-rolling oily sludge

Substanzen

SewageSteelIronOils

Autor:innen und Institutionen

  • School of Energy Science and Engineering, Central South University, Changsha 410083, China.
  • National Engineering Research Center of Sintering and Pelletizing Equipment System, Zhongye Changtian International Engineering Co., Ltd, 410205 Changsha, China.
  • School of Energy Science and Engineering, Central South University, Changsha 410083, China. Electronic address: jpyang@csu.edu.cn.

Förderung

  • National Natural Science Foundation of China National Outstanding Youth Science Fund Project
  • National Natural Science Foundation of China
  • Natural Science Foundation of Hunan Province
  • Science and Technology Program of Hunan Province

Zitieren

APA

Li, H., Xie, B., Zhu, X., Li, Q., & Yang, J. (2023). Erosion behaviour of rotary kiln refractory and its effects on ringing during steel-rolling oily sludge incineration. Waste Management, 164, 162-170. https://doi.org/10.1016/j.wasman.2023.04.005

Vancouver

Li H, Xie B, Zhu X, Li Q, Yang J. Erosion behaviour of rotary kiln refractory and its effects on ringing during steel-rolling oily sludge incineration. Waste Management. 2023;164:162-170. doi:10.1016/j.wasman.2023.04.005

BibTeX
@article{Li2023,
  author = {Li, Hailong and Xie, Bin and Zhu, Xiaolei and Li, Qian and Yang, Jianping},
  title = {Erosion behaviour of rotary kiln refractory and its effects on ringing during steel-rolling oily sludge incineration},
  journal = {Waste Management},
  year = {2023},
  volume = {164},
  pages = {162--170},
  doi = {10.1016/j.wasman.2023.04.005}
}
Kostenlos starten →