Fachartikel in der Zeitschrift The Journal of Prosthetic Dentistry, 2026-06. Verfasst von Aya Fawzy und 2 weiteren Autor:innen. Beteiligte Einrichtung: MSc student, Department of Fixed Prosthodontics, Faculty of Dentistry, Beni-Suef University, Beni-Suef, Egypt. Hauptthemen laut MEDLINE: Crowns, Polyethylene Glycols, Dental Prosthesis, Implant-Supported, Ketones. Die Arbeit wurde bisher 2-mal zitiert (Crossref) und nennt 50 Literaturangaben.
Abstract (Originalsprache)
STATEMENT OF PROBLEM: Polyetheretherketone (PEEK) can be adopted as a coping material for implant-supported crowns. However, data on the fracture resistance of PEEK implant-supported posterior crowns produced by different fabrication techniques are scarce. PURPOSE: The purpose of this in vitro study was to evaluate the effect of different fabrication techniques on the fracture resistance of PEEK implant-supported posterior crowns. MATERIAL AND METHODS: Thirty implants were placed in autopolymerizing acrylic resin blocks, with implant abutments positioned on each implant. Thirty PEEK copings were fabricated and assigned to 3 groups (n=10) depending on the fabrication technique: group MP, milled from a reinforced PEEK disk; group PP, heat pressed from PEEK granules; and group AMP, additively manufactured from PEEK filaments. All PEEK copings were veneered with a nanohybrid composite resin in the form of the maxillary right premolar. Then, a composite resin cement was used to cement the crowns to the implant abutments. All crowns underwent cyclic loading in a mastication simulator (1 200 000 cycles, 1.7 Hz, and 50 N). Fracture resistance was determined by using a universal testing machine, and the failure mode was recorded by using a stereomicroscope at ×15 magnification. A representative fractured crown from each group was assessed under a scanning electron microscope (SEM) at ×1000 magnification. Data were analyzed by using 1-way analysis of variance and the pairwise Tukey (HSD) tests (α=.05). RESULTS: No debonding, chipping, or fractures were detected after cyclic loading. The mean ±standard deviation fracture load values after cyclic loading were 1047 ±108 N for the MP group, 762 ±78 N for the PP group, and 647 ±65 N for the AMP group. Statistically significant differences in fracture resistance were observed among all groups (F=56.77, P
Schlagwörter
MeSH-Schlagwörter (MEDLINE)
Substanzen
Autor:innen und Institutionen
- MSc student, Department of Fixed Prosthodontics, Faculty of Dentistry, Beni-Suef University, Beni-Suef, Egypt.
- Associate Professor, Department of Fixed Prosthodontics, Faculty of Dentistry, Beni-Suef University, Beni-Suef, Egypt.
- Professor, Department of Fixed Prosthodontics, Faculty of Dentistry, Beni-Suef University, Beni-Suef, Egypt. Electronic address: mazen.ahmed@dent.bsu.edu.eg.
Zitieren
APA
Fawzy, A., Radawn, M., & Attia, M. A. (2026). Effect of different fabrication techniques on the fracture resistance of polyetheretherketone implant-supported posterior crowns: An in vitro study. The Journal of Prosthetic Dentistry, 135(6), e132-e139. https://doi.org/10.1016/j.prosdent.2025.12.013
Vancouver
Fawzy A, Radawn M, Attia MA. Effect of different fabrication techniques on the fracture resistance of polyetheretherketone implant-supported posterior crowns: An in vitro study. The Journal of Prosthetic Dentistry. 2026;135(6):e132-e139. doi:10.1016/j.prosdent.2025.12.013
BibTeX
@article{Fawzy2026,
author = {Fawzy, Aya and Radawn, Mohamed and Attia, Mazen A},
title = {Effect of different fabrication techniques on the fracture resistance of polyetheretherketone implant-supported posterior crowns: An in vitro study},
journal = {The Journal of Prosthetic Dentistry},
year = {2026},
volume = {135},
number = {6},
pages = {e132--e139},
doi = {10.1016/j.prosdent.2025.12.013}
}
EUVIMED