Comparison of bond strength to three restorative materials after contamination and the use of two cleaning agents
The Journal of Prosthetic Dentistry · 2025-04 · 133 (4) · 1047-1053
DOI: 10.1016/j.prosdent.2023.06.002 ↗Kurz gefasst
Vergleichsstudie in der Zeitschrift The Journal of Prosthetic Dentistry, 2025-04. Verfasst von Christine Yazigi und 2 weiteren Autor:innen. Beteiligte Einrichtung: Assistant Professor, Department of Prosthodontics, Propaedeutics, and Dental Materials, School of Dentistry, Christian-Albrechts University at Kiel, …. Hauptthemen laut MEDLINE: Dental Bonding, Decontamination, Dental Materials. Die Arbeit wurde bisher 11-mal zitiert (Crossref) und nennt 38 Literaturangaben.
Abstract (Originalsprache)
STATEMENT OF PROBLEM: Scientific data on the decontamination effectiveness of a newly introduced cleaning agent are lacking. PURPOSE: The purpose of this in vitro study was to evaluate and compare the tensile bond strength (TBS) of 3 different restorative bonding surfaces after contamination with saliva following different cleaning protocols. MATERIAL AND METHODS: A total of 192 disk specimens were made out of 3 materials (n=64); Katana Avencia (A), Katana Zirconia (Z), and e.max CAD (L). The bonding surfaces of all disks were polished, steam cleaned, and then pretreated by following the recommended protocol for each material. The specimens of each group were divided into 4 subgroups (n=16). The first subgroup served as the reference (R), where no contamination was applied. The 3 other subgroups were contaminated with saliva and subsequently rinsed with water for 20 seconds and dried with oil- and water-free air spray. They were then either not treated with any cleaning method (0), cleaned with Katana Cleaner (K), or cleaned with Ivoclean (I). The bonding surfaces of the specimens were perpendicularly luted to plexiglass tubes filled with dual-polymerizing composite resin (Clearfil DC Core) with resin cement (Panavia V5) after the recommended surface conditioning. Each subgroup was further subdivided into 2 groups: stored in 37 °C water for 3 days or subjected to thermal-cyclic loading for 150 days with 37 500 thermal cycles (7500 per month), temperature 5 to 55 °C, and dwell time of 30 seconds. All specimens were subjected to TBS testing in a universal testing machine. Three-way ANOVA was applied. A significant interaction (P
Schlagwörter
MeSH-Schlagwörter (MEDLINE)
Substanzen
Autor:innen und Institutionen
- Assistant Professor, Department of Prosthodontics, Propaedeutics, and Dental Materials, School of Dentistry, Christian-Albrechts University at Kiel, Kiel, Schleswig-Holstein, Germany. Electronic address: cyazigi@proth.u…
- Professor and Chairman, Department of Prosthodontics, Propaedeutics, and Dental Materials, School of Dentistry, Christian-Albrechts University at Kiel, Kiel, Schleswig-Holstein, Germany.
- Senior Lecturer, Department of Prosthodontics, Propaedeutics, and Dental Materials, School of Dentistry, Christian-Albrechts University at Kiel, Kiel, Schleswig-Holstein, Germany.
Zitieren
APA
Yazigi, C., Kern, M., & Chaar, M. S. (2025). Comparison of bond strength to three restorative materials after contamination and the use of two cleaning agents. The Journal of Prosthetic Dentistry, 133(4), 1047-1053. https://doi.org/10.1016/j.prosdent.2023.06.002
Vancouver
Yazigi C, Kern M, Chaar MS. Comparison of bond strength to three restorative materials after contamination and the use of two cleaning agents. The Journal of Prosthetic Dentistry. 2025;133(4):1047-1053. doi:10.1016/j.prosdent.2023.06.002
BibTeX
@article{Yazigi2025,
author = {Yazigi, Christine and Kern, Matthias and Chaar, M Sad},
title = {Comparison of bond strength to three restorative materials after contamination and the use of two cleaning agents},
journal = {The Journal of Prosthetic Dentistry},
year = {2025},
volume = {133},
number = {4},
pages = {1047--1053},
doi = {10.1016/j.prosdent.2023.06.002}
}
EUVIMED