Fabrication and characterization of GO/CMC hydrogels: Composition-dependent swelling
Next Materials · 2026-10 · 13 · 103751
DOI: 10.1016/j.nxmate.2026.103751 ↗Kurz gefasst
Fachartikel in der Zeitschrift Next Materials, 2026-10. Verfasst von Chahat und 1 weiteren Autor:innen. Die Arbeit nennt 54 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).
Abstract (Originalsprache)
Carboxymethyl cellulose (CMC) hydrogels swell readily, but their network is mechanically weak and their swelling is difficult to control. To address this, graphene oxide (GO) was incorporated into a CMC matrix, and GO/CMC composite hydrogel beads were prepared by a simple, low-cost route using FeCl₃ as an ionic crosslinker. GO loadings of 0.05, 0.1, 0.2 and 0.3 g were used with a fixed amount of CMC. The formation of GO was confirmed by Raman spectroscopy, which showed the characteristic D and G bands with an I D /I G ratio of about 0.93, and by XRD, which showed an interlayer spacing of 7.46 Å. FTIR of a FeCl₃-crosslinked CMC control showed a shift of the asymmetric carboxylate band from 1589 to 1637 cm⁻¹ and a broad low-wavenumber Fe–O absorption, confirming Fe³ ⁺ binding to CMC. In the composites, FTIR indicated that the functional groups of both components were retained and that the carboxyl band shifted from 1728 cm⁻¹ at 0.05 g GO to 1591–1599 cm⁻¹ at higher loadings, consistent with carboxylate-mediated Fe³ ⁺ crosslinking. The GO reflection disappeared in the XRD patterns of all composites, pointing to exfoliated GO dispersed within a largely amorphous network, while UV–visible spectra confirmed the presence of GO through its n–π* band at 297–299 nm. FE-SEM revealed a progressive change from a smooth, CMC-like surface at low GO loading to layered and increasingly porous morphologies at higher loadings, and EDS confirmed carbon, oxygen and sodium as the main elements. All GO/CMC beads swelled more than a CMC-only control (363.8 ± 1.3%): swelling was highest at 0.05 g GO (1302.6 ± 4.2%) and decreased, with an intermediate rise at 0.2 g, to 442.0 ± 3.5% at 0.3 g GO (one-way ANOVA, p < 0.001), indicating a more constrained network at higher GO content. The beads were also pH-responsive: swelling remained comparatively stable at pH 4 and pH 7 but rose to about 149% after 5 h at pH 9. Overall, GO loading offers a simple means of tuning the structure, morphology and swelling behaviour of CMC hydrogel beads.
Zitieren
APA
Chahat, & Saxena, P. (2026). Fabrication and characterization of GO/CMC hydrogels: Composition-dependent swelling. Next Materials, 13, 103751. https://doi.org/10.1016/j.nxmate.2026.103751
Vancouver
Chahat, Saxena P. Fabrication and characterization of GO/CMC hydrogels: Composition-dependent swelling. Next Materials. 2026;13:103751. doi:10.1016/j.nxmate.2026.103751
BibTeX
@article{Chahat2026,
author = {Chahat and Saxena, Prachi},
title = {Fabrication and characterization of GO/CMC hydrogels: Composition-dependent swelling},
journal = {Next Materials},
year = {2026},
volume = {13},
pages = {103751},
doi = {10.1016/j.nxmate.2026.103751}
}