Fabrication and wetting characteristics of copper thin film: An active layer for SPR-based sensor applications
Journal of Science: Advanced Materials and Devices · 2025-03 · 10 (1) · 100839
DOI: 10.1016/j.jsamd.2024.100839 ↗Kurz gefasst
Fachartikel in der Zeitschrift Journal of Science: Advanced Materials and Devices, 2025-03. Verfasst von Mohammad Kamal Hossain und 4 weiteren Autor:innen. Die Arbeit wurde bisher 5-mal zitiert (Crossref) und nennt 55 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: King Fahd University of Petroleum & Minerals.
Abstract (Originalsprache)
In this work, a simple and two-step process was demonstrated to develop multifunctional Cu-based thin �lms that would be suitable for thin �lm photoactive devices. Cu thin �lms on quartz glass substrates were prepared by sputtering technique followed by a thermal treatment. The samples were annealed at high temperatures such as 200, 400, and 600°C for 2 hrs in a tubular furnace. Surface topography was investigated by a high-resolution scanning electron microscope (FESEM) and SEM-aided energy dispersion spectroscopy (EDS). At high temperatures, the thin �lms were found to have clusters and voids. Detailed studies on optical properties such as UV-vis absorptions, energy band gaps and Urbach energies have been carried out. A red shift in absorption edges (from 464 to 616 nm), a decrease in energy band gaps (from 2.38 to 1.54 eV) and an increase in Urbach energies (from 193 to 272 meV) were observed for those samples annealed at higher temperatures. Sessile drop tests were carried out to �nd the wetting contact angle and demonstrate the hydrophobicity of the thin �lm of pristine Cu and of those treated at high temperatures. Sessile drop tests were carried out to �nd the wetting contact angle (WCA) and demonstrate the hydrophobicity of the thin �lm of pristine Cu and of those treated at high temperatures. An approximate WCA of 71.9° was determined for the Cu thin �lm. After the samples were treated at 200°C and 400°C, respectively, the surface became more hydrophobic by 92.4° and 85.2°. Nevertheless, the same thin �lm's WCA was decreased and its hydrophilicity increased during additional annealing. Cu-based thin �lms have been suggested as the active layer in an SPR sensor model, and the spectrum and angular resolved re�ectance properties have been thoroughly investigated. At spectral wavelengths of 600, 700, and 800 nm, the optimum thickness of Cu thin �lm was determined to be 40 nm at SPR angles of 44.7°, 42.7°, and 42.15°.
Förderung
- King Fahd University of Petroleum & Minerals
Zitieren
APA
Hossain, M. K., Aljishi, A., Khan, F., Ul-Hamid, A., & Rahman, M. M. (2025). Fabrication and wetting characteristics of copper thin film: An active layer for SPR-based sensor applications. Journal of Science: Advanced Materials and Devices, 10(1), 100839. https://doi.org/10.1016/j.jsamd.2024.100839
Vancouver
Hossain MK, Aljishi A, Khan F, Ul-Hamid A, Rahman MM. Fabrication and wetting characteristics of copper thin film: An active layer for SPR-based sensor applications. Journal of Science: Advanced Materials and Devices. 2025;10(1):100839. doi:10.1016/j.jsamd.2024.100839
BibTeX
@article{Hossain2025,
author = {Hossain, Mohammad Kamal and Aljishi, Abdullah and Khan, Firoz and Ul-Hamid, Anwar and Rahman, Md Mosaddequr},
title = {Fabrication and wetting characteristics of copper thin film: An active layer for SPR-based sensor applications},
journal = {Journal of Science: Advanced Materials and Devices},
year = {2025},
volume = {10},
number = {1},
pages = {100839},
doi = {10.1016/j.jsamd.2024.100839}
}
EUVIMED