Extraction of W, V, and As from spent SCR catalyst by alkali pressure leaching and the pressure leaching mechanism
Journal of Environmental Management · 2023-12 · 347 · 119107
DOI: 10.1016/j.jenvman.2023.119107 ↗Kurz gefasst
Fachartikel in der Zeitschrift Journal of Environmental Management, 2023-12. Verfasst von Jinlong Liu und 9 weiteren Autor:innen. Beteiligte Einrichtung: CAS Key Laboratory of Green Process and Engineering, National Engineering Research Center of Green Recycling for Strategic Metal Resources, Institute…. Hauptthemen laut MEDLINE: Alkalies, Titanium. Die Arbeit wurde bisher 20-mal zitiert (Crossref) und nennt 36 Literaturangaben.
Abstract (Originalsprache)
Spent selective catalytic reduction (SCR) catalysts are environmentally hazardous and resource-enriching. In this work, V, W, and As in a spent SCR catalyst was extracted by alkali pressure leaching. Results showed that the V, W, and As were loaded on the anatase TiO2 crystal grains as amorphous oxides. The optimum pressure leaching conditions were NaOH concentration of 20 wt%, reaction temperature of 180 °C, reaction time of 120 min, L/S of 10 mL/g, and stirring speed of 300 rpm. The leaching efficiency of W, V, and As reached 98.83%, 100%, and 100%, respectively. The experiment revealed the preferential leaching of V and As rather than W, and the leaching mechanisms of V, W, and As were studied through experiment and density functional theory (DFT). The leaching kinetics of W conformed to a variant of the shrinking core model and the leaching process of W is controlled by both chemical reactions and diffusion processes. During the leaching process, Na2Ti2O4(OH)2 product powder layer was generated, which affects the mass transfer of W. The destruction of the TiO2 skeleton in the spent SCR catalyst is essential for adequate W extraction, especially for the extraction of W embedded in the TiO2 lattice. The DFT simulation result indicated that the V and As loaded onto the TiO2 support are easier to absorb hydroxide ions rather than W, and the leaching reaction energy of V and As was lower than W, As, and V has leaching priority over the leaching of W. Furthermore, an anatase TiO2 photocatalyst with the {001} crystal surface exposed was successfully prepared from the alkali pressure leaching residue. This work provides theoretical support for the metal leaching and utilization of spent SCR catalysts via alkali pressure leaching.
Schlagwörter
MeSH-Schlagwörter (MEDLINE)
Stichwörter der Autor:innen
Substanzen
Autor:innen und Institutionen
- CAS Key Laboratory of Green Process and Engineering, National Engineering Research Center of Green Recycling for Strategic Metal Resources, Institute of Process Engineering, Chinese Academy of Sciences, Beijing, 100190,…
- Hangzhou Yanqu Information Technology Co., Ltd. Y2, 2nd Floor, Building 2, Xixi Legu Creative Pioneering Park, No. 712 Wen'er West Road, Xihu District, Hangzhou City, Zhejiang Province, 310003, P.R.O.C.
Zitieren
APA
Liu, J., Wang, C., Hou, X., Li, H., Wang, X., Hu, W., Ge, T., Zhang, J., Zhu, G., & Xie, H. (2023). Extraction of W, V, and As from spent SCR catalyst by alkali pressure leaching and the pressure leaching mechanism. Journal of Environmental Management, 347, 119107. https://doi.org/10.1016/j.jenvman.2023.119107
Vancouver
Liu J, Wang C, Hou X, Li H, Wang X, Hu W, et al. Extraction of W, V, and As from spent SCR catalyst by alkali pressure leaching and the pressure leaching mechanism. Journal of Environmental Management. 2023;347:119107. doi:10.1016/j.jenvman.2023.119107
BibTeX
@article{Liu2023,
author = {Liu, Jinlong and Wang, Chenye and Hou, Xinjuan and Li, Huiquan and Wang, Xingrui and Hu, Wenbin and Ge, Te and Zhang, Jianbo and Zhu, Ganyu and Xie, Haijiao},
title = {Extraction of W, V, and As from spent SCR catalyst by alkali pressure leaching and the pressure leaching mechanism},
journal = {Journal of Environmental Management},
year = {2023},
volume = {347},
pages = {119107},
doi = {10.1016/j.jenvman.2023.119107}
}
EUVIMED