Fracture resistance of 3D printed resin-based permanent ceramic fixed dental prostheses after thermocycling
Journal of Dentistry · 2026-11 · 174 · 106917
DOI: 10.1016/j.jdent.2026.106917 ↗Kurz gefasst
Vergleichsstudie in der Zeitschrift Journal of Dentistry, 2026-11. Verfasst von Safa Ozer und 2 weiteren Autor:innen. Beteiligte Einrichtung: Department of Prosthodontics, School of Dental Medicine, Bahçeşehir University, Istanbul, Turkey; Department of Prosthodontics, Faculty of Dentistry,…. Hauptthemen laut MEDLINE: Printing, Three-Dimensional, Ceramics, Dental Materials, Denture, Partial, Fixed. Die Arbeit nennt 45 Literaturangaben.
Abstract (Originalsprache)
OBJECTIVES: Three-dimensionally (3D) printed resin-based permanent ceramics produced using additive manufacturing have recently gained considerable interest as potential restorative materials for fixed prostheses. However, limited evidence is available regarding their long-term mechanical performance following thermocycling. The aim of this study was to evaluate the effect of different thermocycling durations on the fracture resistance of 3D-printed bar-type fixed dental prosthesis (FDP) specimens. METHODS: Forty-eight bar-shaped, three-unit FDP specimens (5 × 5 × 30 mm), each containing a 4 × 4 mm² U-shaped connector, were fabricated using 3D-printed resin-based permanent ceramic. The specimens were divided into four groups according to ageing duration: unaged, 1, 3, and 12 months of thermocycling. Fracture load (N) data were analysed using non-parametric statistical methods. Group comparisons were performed using the Kruskal-Wallis test with epsilon-squared (ε²) effect size estimation, and the Jonckheere-Terpstra test was applied to evaluate the ordered trend across thermocycling durations. RESULTS: Group comparisons showed no statistically significant differences in fracture load among ageing durations (Kruskal-Wallis, p = 0.168), with a small effect size (ε² = 0.047). However, the Jonckheere-Terpstra test indicated a significant decreasing trend in fracture load with an increase in thermocycling duration (Z = -2.135, p = 0.033). CONCLUSIONS: Although no statistically significant group differences were observed, effect size analysis and regression trends indicated that long-term thermocycling may gradually reduce the fracture resistance of 3D-printed resin-based permanent ceramic FDPs. CLINICAL SIGNIFICANCE: 3D-printed resin-based permanent ceramic FDPs can provide satisfactory initial fracture resistance; however, the mechanical strength reduction tendency following long-term ageing should be considered for clinical applications over extended durations.
Schlagwörter
MeSH-Schlagwörter (MEDLINE)
Stichwörter der Autor:innen
Substanzen
Autor:innen und Institutionen
- Department of Prosthodontics, School of Dental Medicine, Bahçeşehir University, Istanbul, Turkey; Department of Prosthodontics, Faculty of Dentistry, Istanbul Health and Technology University, Istanbul, Turkey. Electron…
- Department of Prosthodontics, Faculty of Dentistry, Istanbul Health and Technology University, Istanbul, Turkey.
Zitieren
APA
Ozer, S., Akgun, B. A., & Cakan, U. (2026). Fracture resistance of 3D printed resin-based permanent ceramic fixed dental prostheses after thermocycling. Journal of Dentistry, 174, 106917. https://doi.org/10.1016/j.jdent.2026.106917
Vancouver
Ozer S, Akgun BA, Cakan U. Fracture resistance of 3D printed resin-based permanent ceramic fixed dental prostheses after thermocycling. Journal of Dentistry. 2026;174:106917. doi:10.1016/j.jdent.2026.106917
BibTeX
@article{Ozer2026,
author = {Ozer, Safa and Akgun, Begum Atasoyu and Cakan, Umut},
title = {Fracture resistance of 3D printed resin-based permanent ceramic fixed dental prostheses after thermocycling},
journal = {Journal of Dentistry},
year = {2026},
volume = {174},
pages = {106917},
doi = {10.1016/j.jdent.2026.106917}
}