Suppressing lattice oxygen-induced interfacial degradation via a multifunctional siloxane additive for 4.8 V LRMO‖Li batteries
Journal of Colloid and Interface Science · 2026-11 · 722 · 141007
DOI: 10.1016/j.jcis.2026.141007 ↗Kurz gefasst
Fachartikel in der Zeitschrift Journal of Colloid and Interface Science, 2026-11. Verfasst von Guiqiang Ai und 4 weiteren Autor:innen. Beteiligte Einrichtung: School of Physics and Materials Science, Nanchang University, Nanchang 330031, China. Die Arbeit wurde bisher 2-mal zitiert (Crossref) und nennt 34 Literaturangaben. Gefördert von: Jiangxi Provincial Natural Science Foundation, China Postdoctoral Science Foundation.
Abstract (Originalsprache)
Lithium-rich manganese-based oxides (LRMO) are promising cathodes for high-energy-density lithium-metal batteries owing to their high operating voltage and large reversible capacity, but suffer from severe interfacial degradation at high voltages (≥4.8 V), primarily triggered by lattice oxygen release, electrolyte oxidation, and HF-induced corrosion. Herein, we design a multifunctional siloxane-based electrolyte additive, 1,3,5-tris(3,3,3-trifluoropropyl)methylcyclotrisiloxane (TFSO), to regulate these coupled degradation processes. TFSO simultaneously acts as an oxygen scavenger and HF trap, suppressing lattice oxygen reactivity while converting HF into stable SiF/SiO species. Meanwhile, it promotes the formation of robust, inorganic-rich CEI/SEI layers, enabling dual interfacial stabilization and uniform lithium deposition. In addition, TFSO reconstructs the Li+ solvation structure, reducing solvent participation in interfacial side reactions. As a result, the LRMO‖Li cell achieves 92.7% capacity retention after 300 cycles at 4.8 V, along with excellent wide-temperature performance (82.7% at 55 °C and 160 mAh g-1 at 0 °C). This work highlights an effective electrolyte design strategy for mitigating oxygen-triggered interfacial degradation in high-voltage lithium metal batteries.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- School of Physics and Materials Science, Nanchang University, Nanchang 330031, China.
- School of Physics and Materials Science, Nanchang University, Nanchang 330031, China. Electronic address: yangxuerui@ncu.edu.cn.
- School of Physics and Materials Science, Nanchang University, Nanchang 330031, China. Electronic address: ngzhou@ncu.edu.cn.
Förderung
- Jiangxi Provincial Natural Science Foundation
- China Postdoctoral Science Foundation
Zitieren
APA
Ai, G., Wu, C., Su, R., Yang, X., & Zhou, N. (2026). Suppressing lattice oxygen-induced interfacial degradation via a multifunctional siloxane additive for 4.8 V LRMO‖Li batteries. Journal of Colloid and Interface Science, 722, 141007. https://doi.org/10.1016/j.jcis.2026.141007
Vancouver
Ai G, Wu C, Su R, Yang X, Zhou N. Suppressing lattice oxygen-induced interfacial degradation via a multifunctional siloxane additive for 4.8 V LRMO‖Li batteries. Journal of Colloid and Interface Science. 2026;722:141007. doi:10.1016/j.jcis.2026.141007
BibTeX
@article{Ai2026,
author = {Ai, Guiqiang and Wu, Changquan and Su, Rui and Yang, Xuerui and Zhou, Naigen},
title = {Suppressing lattice oxygen-induced interfacial degradation via a multifunctional siloxane additive for 4.8 V LRMO‖Li batteries},
journal = {Journal of Colloid and Interface Science},
year = {2026},
volume = {722},
pages = {141007},
doi = {10.1016/j.jcis.2026.141007}
}