Fachartikel in der Zeitschrift International Dental Journal, 2026-10. Verfasst von Chanho Kim und 1 weiteren Autor:innen. Der Volltext ist frei zugänglich (Open Access, CC BY-NC-ND 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

AIM or PURPOSE To evaluate if high-speed sintered zirconia crowns are clinically acceptable, by assessing mechanical properties and marginal fit of zirconia crowns before and after thermomechanical aging. MATERIALS and METHODS Maxillary second molar phantom tooth was prepared and scanned with intraoral scanner. The data was used to replicate a cobalt-chromium model using a metal 3D printer. Single zirconia crowns were designed using CAD software and milled from 4Y-PSZ zirconia blocks. High-speed sintering was carried out at a peak temperature of 1550°C with a holding time of 5 minutes, resulting in a total sintering time of approximately 20 minutes. Thermocycling and mechanical loading were performed to simulate thermomechanical aging. RESULTS Thermomechanical aging affected the marginal and occlusal fit, whereas no significant differences were observed in the axial wall and line angle regions. Fracture strength significantly decreased after thermomechanical aging. SEM observations showed relatively larger grains and more densely packed microstructure after thermomechanical aging. XRD analysis showed monoclinic phase fraction increase after aging, suggesting that thermomechanical aging may promoted tetragonal-to-monoclinic transformation. CONCLUSIONS Marginal and occlusal gaps increased after thermomechanical aging. However, the mean gap values remained within the clinically acceptable threshold of 120 µm. Fracture strength decreased after thermomechanical aging. Nevertheless, the fracture load after aging remained higher than the maximum molar bite force, indicating sufficient load-bearing capacity. Microstructural analysis revealed a tendency toward increased grain size after aging, while XRD analysis demonstrated an increase in the monoclinic phase fraction. Zirconia crowns fabricated using high-speed sintering maintained clinically acceptable fit and sufficient mechanical performance after thermomechanical aging.

Zitieren

APA

Kim, C., & Doh, R. (2026). Mechanical Properties of high-speed sintered Zirconia Crowns After Thermomechanical Aging. International Dental Journal, 76, 110487. https://doi.org/10.1016/j.identj.2026.110487

Vancouver

Kim C, Doh R. Mechanical Properties of high-speed sintered Zirconia Crowns After Thermomechanical Aging. International Dental Journal. 2026;76:110487. doi:10.1016/j.identj.2026.110487

BibTeX
@article{Kim2026,
  author = {Kim, Chanho and Doh, Remee},
  title = {Mechanical Properties of high-speed sintered Zirconia Crowns After Thermomechanical Aging},
  journal = {International Dental Journal},
  year = {2026},
  volume = {76},
  pages = {110487},
  doi = {10.1016/j.identj.2026.110487}
}
Kostenlos starten →