Bonding performance using all-in-one adhesive on conventional, self-glazed, 3D-printed zirconia
International Dental Journal · 2026-10 · 76 · 110486
DOI: 10.1016/j.identj.2026.110486 ↗Kurz gefasst
Fachartikel in der Zeitschrift International Dental Journal, 2026-10. Verfasst von Sadia Manzoor und 3 weiteren Autor:innen. Der Volltext ist frei zugänglich (Open Access, CC BY-NC-ND 4.0).
Abstract (Originalsprache)
AIM or PURPOSE Evaluate resin-zirconia shear bond strength and physical characteristics of milled and additively manufactured DLP and self-glazed zirconia after surface treatment and thermocycling aging by using an all-in-one adhesive. MATERIALS and METHODS Resin stub on zirconia specimens (∼⌀16.0×1.0 mm thickness) were fabricated on 3Y, translucent 4Y-PSZ, 5Y-PSZ, additively manufactured self-glazed zirconia, and 3D-printed zirconia with a homemade DLP 3D-printer on loaded 80 wt% 3Y zirconia photosensitive slurry, 42 vol% solid phase content. Samples were divided into groups: Group A, polished zirconia; Group B, sandblasted zirconia (50 μm Al2O3). Groups were subdivided into two groups: with primer or without primer all-in-one primer adhesive on specimens. Surface roughness and morphology were measured by profilometer and SEM. Contact angle and surface free energy was evaluated. Self-adhesive resin cement cylinder (∼Ø2.65 mm, h=2 mm) was built on zirconia and subjected to shear bond strength test (n=18) after 24 hrs of bonding and 1000, 5000, and 10000 cycles of thermocycling. Statistical differences was studied by one-way ANOVA and Tukey’s HSD post hoc multiple-comparison test. Material type, primer application, and (surface treatment or thermocycling) on shear bond strength were analyzed by Three-way ANOVA. RESULTS Sandblasting and priming increased surface free energy, DLP exhibited lowest water contact angles and largest surface free energy. Primer was significant factor influencing Shear Bond Strength (p < 0.001), followed by sandblasting (p < 0.001), zirconia type alone exhibited no impact. CONCLUSIONS Primer application would be vital for durable adhesion, and its effect is enhanced by sandblasting and moderated by thermocycling if all-in-one adhesive is used.
Zitieren
APA
Manzoor, S., Zhao, W., Ding, H., & Tsoi, J. K. H. (2026). Bonding performance using all-in-one adhesive on conventional, self-glazed, 3D-printed zirconia. International Dental Journal, 76, 110486. https://doi.org/10.1016/j.identj.2026.110486
Vancouver
Manzoor S, Zhao W, Ding H, Tsoi JKH. Bonding performance using all-in-one adhesive on conventional, self-glazed, 3D-printed zirconia. International Dental Journal. 2026;76:110486. doi:10.1016/j.identj.2026.110486
BibTeX
@article{Manzoor2026,
author = {Manzoor, Sadia and Zhao, wuyuan and Ding, Hao and Tsoi, James Kit Hon},
title = {Bonding performance using all-in-one adhesive on conventional, self-glazed, 3D-printed zirconia},
journal = {International Dental Journal},
year = {2026},
volume = {76},
pages = {110486},
doi = {10.1016/j.identj.2026.110486}
}
EUVIMED