Comparative durability of NaOH-activated and Na2SiO3-activated geopolymer for Pb solidification/stabilization under chemical attack

Xiyao Zheng, Liang Li, Guanglei Yu, Jun Wu, Xiuli Du

Environmental Research · 2026-06 · 299 · 124233

DOI: 10.1016/j.envres.2026.124233 ↗

Kurz gefasst

Vergleichsstudie in der Zeitschrift Environmental Research, 2026-06. Verfasst von Xiyao Zheng und 4 weiteren Autor:innen. Beteiligte Einrichtung: Key Laboratory of Urban Security and Disaster Engineering, Beijing Univ. of Technology, Ministry of Education, Beijing, 100124, China. Electronic add…. Hauptthemen laut MEDLINE: Lead, Sodium Hydroxide, Silicates, Polymers. Die Arbeit wurde bisher 2-mal zitiert (Crossref) und nennt 36 Literaturangaben. Gefördert von: National Natural Science Foundation of China.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Rapid industrial development and site reuse have increased the risk of lead (Pb) pollution under aggressive chemical conditions. Solidification/stabilization is widely applied to immobilize Pb by reducing its mobility through physical encapsulation and chemical stabilization. One-part geopolymer synthesized from industrial by-products and solid alkaline activators has attracted attention due to their improved safety and practical applicability compared with conventional two-part systems, while their long-term durability and Pb immobilization performance under chemical attack remain insufficiently understood. In this study, one-part NaOH-activated geopolymer (NHG) and Na2SiO3-activated geopolymer (NSG), synthesized from ground granulated blast furnace slag and fly ash, were evaluated as binders for Pb immobilization. Pb-doped NHG and Pb-doped NSG were immersed in H2SO4, HCl, Na2SO4, and NaCl solutions, with water immersion used as a reference. Durability was assessed through macroscopic appearance, mass loss, unconfined compressive strength (UCS), durability coefficient, and Pb leaching behavior, while microstructure evolution and Pb distribution were examined by SEM-EDS. The results showed that chemical erosion severity follows the order H2SO4 > HCl > Na2SO4 > NaCl, with a corresponding ion aggressiveness sequence H+ > SO42- > Cl- > Na+. Before immersion, NSG exhibited a much higher initial UCS than NHG. At Pb0.8, NHG reached 24.37 MPa, whereas NSG achieved 68.15 MPa. Under chemical attack, particularly in acidic environments, NSG experienced faster UCS degradation. In contrast, NHG showed superior long-term durability, characterized by better UCS retention and lower degradation. Despite these differences, Pb leaching concentrations remained below 5 mg/L under all tested conditions. SEM-EDS observations indicated that durability differences were associated with distinct binding gels, with NHG governed by a network-like C-S-H gel and NSG dominated by a gel-like N-A-S-H. Overall, Pb-doped NHG exhibited more favorable comprehensive performance when long-term durability was considered.

Schlagwörter

MeSH-Schlagwörter (MEDLINE)

LeadSodium HydroxideSilicatesPolymers

Stichwörter der Autor:innen

Chemical attackChemical erosion mechanismNa(2)SiO(3)-activated geopolymerNaOH-Activated geopolymerPb contaminants

Substanzen

LeadSodium HydroxideSilicatessodium silicatePolymers

Autor:innen und Institutionen

  • Key Laboratory of Urban Security and Disaster Engineering, Beijing Univ. of Technology, Ministry of Education, Beijing, 100124, China. Electronic address: jsycyjhlgvce@163.com.
  • Key Laboratory of Urban Security and Disaster Engineering, Beijing Univ. of Technology, Ministry of Education, Beijing, 100124, China. Electronic address: liliang@bjut.edu.cn.
  • Key Laboratory of Urban Security and Disaster Engineering, Beijing Univ. of Technology, Ministry of Education, Beijing, 100124, China. Electronic address: yuguanglei1219@163.com.
  • School of Civil Engineering, Shanghai Normal Univ., Shanghai, 201418, China. Electronic address: cvewujun@shnu.edu.cn.
  • Key Laboratory of Urban Security and Disaster Engineering, Beijing Univ. of Technology, Ministry of Education, Beijing, 100124, China. Electronic address: duxiuli@bjut.edu.cn.

Förderung

  • National Natural Science Foundation of China

Zitieren

APA

Zheng, X., Li, L., Yu, G., Wu, J., & Du, X. (2026). Comparative durability of NaOH-activated and Na2SiO3-activated geopolymer for Pb solidification/stabilization under chemical attack. Environmental Research, 299, 124233. https://doi.org/10.1016/j.envres.2026.124233

Vancouver

Zheng X, Li L, Yu G, Wu J, Du X. Comparative durability of NaOH-activated and Na2SiO3-activated geopolymer for Pb solidification/stabilization under chemical attack. Environmental Research. 2026;299:124233. doi:10.1016/j.envres.2026.124233

BibTeX
@article{Zheng2026,
  author = {Zheng, Xiyao and Li, Liang and Yu, Guanglei and Wu, Jun and Du, Xiuli},
  title = {Comparative durability of NaOH-activated and Na2SiO3-activated geopolymer for Pb solidification/stabilization under chemical attack},
  journal = {Environmental Research},
  year = {2026},
  volume = {299},
  pages = {124233},
  doi = {10.1016/j.envres.2026.124233}
}
Kostenlos starten →