Biocompatibility and degradation of PLA reinforced with tungsten disulfide nanotubes for 3D-printed bone scaffold
Biomaterials Advances · 2026
DOI: 10.1016/j.bioadv.2026.214736 ↗Kurz gefasst
Fachartikel in der Zeitschrift Biomaterials Advances, 2026. Verfasst von Ofek Golan und 8 weiteren Autor:innen. Beteiligte Einrichtung: Department of Materials Science and Engineering, Iby and Aladar Fleischman Faculty of Engineering, Tel Aviv University, Tel Aviv 6997801, Israel. Ele…. Hauptthemen laut MEDLINE: Printing, Three-Dimensional, Polyesters, Tissue Scaffolds, Nanotubes. Die Arbeit nennt 117 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Israel Science Foundation, Israel Ministry of Defense, Horizon 2020 Framework Programme.
Abstract (Originalsprache)
Advancements in bone tissue engineering have increased interest in 3D-printed scaffolds for bone regeneration. Polylactic acid (PLA), a biocompatible and biodegradable polyester, is a promising candidate for bone scaffold materials. Reinforcing PLA with inorganic nanotubes of tungsten disulfide (INT-WS2) offers new possibilities for scaffold design. INT-WS2 is an innovative material known for its chemical stability, non-toxicity, and favorable mechanical properties. Integrating PLA with INT-WS2 marks a pioneering development in bone scaffold technology, providing a safer, more effective alternative to other nanofillers, such as TiO₂ nanoparticles and carbon nanotubes, which face challenges related to cytotoxicity and dispersion. This study adds an important aspect to the characterization of this material by investigating the cytocompatibility and hydrolytic degradation effects on 3D-printed samples of PLA reinforced with 0.5 wt% INT-WS2. The samples are proposed as structurally suitable candidate for load-bearing 3D-printed bone scaffolds, with the femur chosen as the upper-limit mechanical benchmark. Controlled hydrolytic degradation of PLA/INT-WS2 samples was conducted over 12 weeks under human-body simulated conditions. Results demonstrated that the material underwent bulk degradation while maintaining mass and surface hardness. Although the ultimate tensile strength progressively decreased to two-thirds of its initial value, potentially allowing gradual loading of the growing bone, it remained significantly higher than the maximum stress experienced by the human femur during normal walking. Furthermore, the PLA/INT-WS2 nanocomposite exhibited non-toxic behavior, promoting cell viability and proliferation. Despite the need for a longer experiment to fully assess the degradation rate, these findings support PLA/INT-WS2 as a promising candidate for tailored 3D-printed bone scaffolds designed for individual patients.
Schlagwörter
MeSH-Schlagwörter (MEDLINE)
Stichwörter der Autor:innen
Substanzen
Autor:innen und Institutionen
- Department of Materials Science and Engineering, Iby and Aladar Fleischman Faculty of Engineering, Tel Aviv University, Tel Aviv 6997801, Israel. Electronic address: ofekgolan1@mail.tau.ac.il.
- Department of Materials Science and Engineering, Iby and Aladar Fleischman Faculty of Engineering, Tel Aviv University, Tel Aviv 6997801, Israel.
- Department of Organic Chemistry, School of Chemistry, Faculty of Exact Sciences, Tel-Aviv University, Tel Aviv 6997801, Israel; The Center for Physics & Chemistry of Living Systems, and Jan Koum Center for Nanoscience a…
- Department of Oral Biology, The Goldschleger School of Dental Medicine, Gray Faculty of Medical & Health Sciences, Tel Aviv University, Tel Aviv 6997801, Israel; The Center for Physics & Chemistry of Living Systems, and…
- Department of Materials Science and Engineering, Iby and Aladar Fleischman Faculty of Engineering, Tel Aviv University, Tel Aviv 6997801, Israel. Electronic address: noala@tauex.tau.ac.il.
Förderung
- Israel Science Foundation
- Israel Ministry of Defense
- Horizon 2020 Framework Programme
- European Research Council
- H2020 European Research Council
Zitieren
APA
Golan, O., Granada, N., Lemesh, L., Azoulay-Ginsburg, S., Netti, F., Altobelli, V., Amir, R. J., Adler-Abramovich, L., & Lachman, N. (2026). Biocompatibility and degradation of PLA reinforced with tungsten disulfide nanotubes for 3D-printed bone scaffold. Biomaterials Advances. https://doi.org/10.1016/j.bioadv.2026.214736
Vancouver
Golan O, Granada N, Lemesh L, Azoulay-Ginsburg S, Netti F, Altobelli V, et al. Biocompatibility and degradation of PLA reinforced with tungsten disulfide nanotubes for 3D-printed bone scaffold. Biomaterials Advances. 2026. doi:10.1016/j.bioadv.2026.214736
BibTeX
@article{Golan2026,
author = {Golan, Ofek and Granada, Noa and Lemesh, Lin and Azoulay-Ginsburg, Salome and Netti, Francesca and Altobelli, Vania and Amir, Roey J and Adler-Abramovich, Lihi and Lachman, Noa},
title = {Biocompatibility and degradation of PLA reinforced with tungsten disulfide nanotubes for 3D-printed bone scaffold},
journal = {Biomaterials Advances},
year = {2026},
doi = {10.1016/j.bioadv.2026.214736}
}