EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Corrosion behavior and mechanisms of 3Cr steel in a high-salinity O2–CO2 environment

Hangbo Hu, Yanming Liu, Minlu Shi, Mingwei Yao, Xianghong Lü, Pan Dai

Surface Science and Technology · 2026-12 · 4 (1)

DOI: 10.1007/s44251-026-00142-8 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Surface Science and Technology, online erschienen am 08.07.2026. Verfasst von Hangbo Hu und 5 weiteren Autor:innen. Die Arbeit wurde bisher 1-mal zitiert (Crossref) und nennt 40 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: The Natural Science Foundation of Shaanxi Province of China, The Innovation Team Funding by Xi’an Shiyou University, The Major Science and Technology Special Project of Xinjiang Uygur Autonomous Region.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

To investigate the corrosion behavior and mechanisms of 3Cr steel under high-salinity, high-Ca 2+ , and O 2 –CO 2 conditions, we simulated the service environment of a western China oilfield (total salinity 250,022 mg/L, Ca 2+ > 15,400 mg/L). Immersion and electrochemical tests were conducted at 120 °C under 0.5 MPa CO 2 with O 2 partial pressures from 0 to 0.4 MPa. The results showed that the uniform corrosion rate increased sharply from 0.6492 mm/a in pure CO 2 to 4.8551 mm/a at 0.4 MPa O 2 , with localized corrosion notably aggravated. It was found that the high Cl − concentration acted as a crystallization inhibitor, forcing the FeCO 3 corrosion product into an amorphous state. In pure CO 2 , the corrosion film displayed a multilayered architecture: a surface crystalline CaCO 3 layer with micropores exhibiting inward/outward growth, an intermediate amorphous FeCO 3 layer, and an inner amorphous Cr-rich oxide layer. This structure was governed by the kinetic dominance of Ca 2+ , which preferentially precipitated as CaCO 3 , thereby suppressing FeCO 3 growth through interfacial competition and localized acidification. With O 2 introduction, the synergistic effect of O 2 , Ca 2+ , and Cl − triggered the formation of a loose, porous Fe 2 O 3 /CaCO 3 composite scale. Notably, 3Cr steel exhibited a weak deposition behavior of CaCO 3 because of both the lower deposition tendency and adhesion strength of CaCO 3 on the amorphous Cr-rich layer. This structural deficiency led to non-uniform film coverage and generated a “small-anode/large-cathode” configuration, accelerating lateral pitting propagation. Although the dense Cr-rich layer effectively hindered Cl − penetration into the substrate, it cannot prevent the expansion of acidified occluded cells. These findings elucidate the synergistic effects of O 2 –CO 2 –Cl − –Ca 2+ on 3Cr steel corrosion and provide a theoretical basis for material selection and protection of tubing steels in oxygenated, high-salinity oil and gas wells.

Förderung

  • The Natural Science Foundation of Shaanxi Province of China
  • The Innovation Team Funding by Xi’an Shiyou University
  • The Major Science and Technology Special Project of Xinjiang Uygur Autonomous Region
  • The Opening Project Fund of Materials Service Safety Assessment Facilities

Zitieren

APA

Hu, H., Liu, Y., Shi, M., Yao, M., Lü, X., & Dai, P. (2026). Corrosion behavior and mechanisms of 3Cr steel in a high-salinity O2–CO2 environment. Surface Science and Technology, 4(1). https://doi.org/10.1007/s44251-026-00142-8

Vancouver

Hu H, Liu Y, Shi M, Yao M, Lü X, Dai P. Corrosion behavior and mechanisms of 3Cr steel in a high-salinity O2–CO2 environment. Surface Science and Technology. 2026;4(1). doi:10.1007/s44251-026-00142-8

BibTeX
@article{Hu2026,
  author = {Hu, Hangbo and Liu, Yanming and Shi, Minlu and Yao, Mingwei and Lü, Xianghong and Dai, Pan},
  title = {Corrosion behavior and mechanisms of 3Cr steel in a high-salinity O2–CO2 environment},
  journal = {Surface Science and Technology},
  year = {2026},
  volume = {4},
  number = {1},
  doi = {10.1007/s44251-026-00142-8}
}