EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Effect of boron and titanium on hot ductility of a low carbon niobium microalloyed steel

Yáiza Montaña, Jacek Komenda, Hans Magnusson, Beatriz Pereda, Jon Arruabarrena

Journal of Iron and Steel Research International · 2026-11 · 33 (11)

DOI: 10.1007/s42243-026-01933-x ↗

Kurz gefasst

Fachartikel in der Zeitschrift Journal of Iron and Steel Research International, online erschienen am 29.09.2026. Verfasst von Yáiza Montaña und 4 weiteren Autor:innen. Die Arbeit nennt 47 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Research Fund for Coal and Steel, Universidad de Navarra.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Hot tensile and compression tests were performed to evaluate the effect of B and Ti on the hot ductility of a low-C Nb-microalloyed steel. Specimens were solution-treated at 1350 °C and cooled at 0.83 °C/s to test temperatures between 750 and 1000 °C. The Nb-microalloyed steel exhibited a wide trough, extending from 950 to 750 °C. The addition of 0.0025 wt.% B improved hot ductility, increasing the reduction of area by more than 10% across the entire temperature range and shifting the trough to 925–800 °C. In the austenitic region, this improvement was attributed to increased grain boundary cohesion caused by B in solid solution and the formation of coarse, non-detrimental BN precipitates, while B also influenced the austenite-to-ferrite transformation kinetics. The simultaneous addition of Ti and B further enhanced hot ductility, narrowing the trough to 850–800 °C and raising the reduction of area above 60%. Detailed characterization using field emission gun scanning electron microscopy and transmission electron microscopy, combined with thermodynamic simulations, revealed that Ti combined with N to form TiN, which increased B in solid solution by reducing BN formation. Additionally, Ti modified Nb precipitation patterns, promoting fewer, coarser (Nb, Ti)(C, N) precipitates at 900 °C. However, at 800 °C, increasing Ti promoted a higher density of fine particles, which deteriorated hot ductility. These results are supported by kinetic simulations. Therefore, the optimum Ti additions correspond to hypo- or stoichiometric ratios with N, where B is protected in solid solution while precipitation effects are minimized.

Förderung

  • Research Fund for Coal and Steel
  • Universidad de Navarra

Zitieren

APA

Montaña, Y., Komenda, J., Magnusson, H., Pereda, B., & Arruabarrena, J. (2026). Effect of boron and titanium on hot ductility of a low carbon niobium microalloyed steel. Journal of Iron and Steel Research International, 33(11). https://doi.org/10.1007/s42243-026-01933-x

Vancouver

Montaña Y, Komenda J, Magnusson H, Pereda B, Arruabarrena J. Effect of boron and titanium on hot ductility of a low carbon niobium microalloyed steel. Journal of Iron and Steel Research International. 2026;33(11). doi:10.1007/s42243-026-01933-x

BibTeX
@article{Montaa2026,
  author = {Montaña, Yáiza and Komenda, Jacek and Magnusson, Hans and Pereda, Beatriz and Arruabarrena, Jon},
  title = {Effect of boron and titanium on hot ductility of a low carbon niobium microalloyed steel},
  journal = {Journal of Iron and Steel Research International},
  year = {2026},
  volume = {33},
  number = {11},
  doi = {10.1007/s42243-026-01933-x}
}
Kostenlos starten →