EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Evaluation of Reduction Behavior of the Acid Pellets Prepared with Sinter-Grade Iron Ore Fines by 55% H2–35% CO–10% N2 and 100% H2

Rijoo Kim, In-kook Suh, Joonho Lee

Journal of Sustainable Metallurgy · 2025-03 · 11 (1) · 300-312

DOI: 10.1007/s40831-025-01005-6 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Journal of Sustainable Metallurgy, online erschienen am 10.02.2025. Verfasst von Rijoo Kim und 2 weiteren Autor:innen. Die Arbeit wurde bisher 8-mal zitiert (Crossref) und nennt 35 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Korea Institute of Energy Technology Evaluation and Planning, Korea Institute for Advancement of Technology.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Hydrogen is receiving much attention as a reducing agent in iron and steel production processes. Hydrogen-based DRI (Direct-Reduced Iron) production in a shaft furnace is currently under development in many countries. However, due to the limited resources for DR-grade pellets, the hydrogen reduction technology of the pellets produced with sinter-grade iron ore fines is highly anticipated. In this study, the reduction characteristics of the acid pellets produced with sinter-grade iron ore fines were investigated by a typical reformed natural gas (55% H 2 –35% CO–10% N 2 ), and 100% H 2 at temperatures ranging from 973 to 1173 K. The lab-made acid pellet exhibited an average cold crushing strength of 335 kg. When the pellets were reduced by 55% H 2 –35% CO–10% N 2 , the degree of metallization was satisfied only at 1173 K. On the other hand, when the pellets were reduced by 100% H 2 , the degree of metallization was acceptable: 93.04 and 95.54% at 1073 and 1173 K, respectively. The reduction time by 100% H 2 at 1073 K was 29 min, whereas that by 55% H 2 –35% CO–10% N 2 at 1173 K was 57 min. Accordingly, the hydrogen reduction process can reduce the reduction time by 51%, although the reduction temperature by 100% H 2 is 100 K lower than that by 55% H 2 –35% CO–10% N 2 . Graphical Abstract

Förderung

  • Korea Institute of Energy Technology Evaluation and Planning
  • Korea Institute for Advancement of Technology

Zitieren

APA

Kim, R., Suh, I., & Lee, J. (2025). Evaluation of Reduction Behavior of the Acid Pellets Prepared with Sinter-Grade Iron Ore Fines by 55% H2–35% CO–10% N2 and 100% H2. Journal of Sustainable Metallurgy, 11(1), 300-312. https://doi.org/10.1007/s40831-025-01005-6

Vancouver

Kim R, Suh I, Lee J. Evaluation of Reduction Behavior of the Acid Pellets Prepared with Sinter-Grade Iron Ore Fines by 55% H2–35% CO–10% N2 and 100% H2. Journal of Sustainable Metallurgy. 2025;11(1):300-312. doi:10.1007/s40831-025-01005-6

BibTeX
@article{Kim2025,
  author = {Kim, Rijoo and Suh, In-kook and Lee, Joonho},
  title = {Evaluation of Reduction Behavior of the Acid Pellets Prepared with Sinter-Grade Iron Ore Fines by 55% H2–35% CO–10% N2 and 100% H2},
  journal = {Journal of Sustainable Metallurgy},
  year = {2025},
  volume = {11},
  number = {1},
  pages = {300--312},
  doi = {10.1007/s40831-025-01005-6}
}
Kostenlos starten →