EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

X-Ray Imaging of Multi-Capillary Formation During Core-Ring Beam Laser Welding of Steel With Different Ring Beam Diameters

Felix Zaiß, John Powell, Michael Haas, Christian Diegel, Klaus Schricker, Jean Pierre Bergmann, Christoph Spurk, Marc Hummel, Alexander Olowinsky, Felix Beckmann, Julian Moosmann, Christian Hagenlocher und 1 weitere

Lasers in Manufacturing and Materials Processing · 2026-09 · 13 (3) · 677-698

DOI: 10.1007/s40516-026-00348-6 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Lasers in Manufacturing and Materials Processing, online erschienen am 20.05.2026. Verfasst von Felix Zaiß und 12 weiteren Autor:innen. Die Arbeit nennt 51 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Universität Stuttgart.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

The shape of the capillary produced during the welding of 1.4301 (X5CrNi18-10, AISI 304) stainless steel at a welding speed of 12 m/min using core-ring-shaped beams delivered through a multi-waveguide fiber was examined by means of synchrotron X-ray imaging. The results show that, under the range of process parameters covered here, ring beams create a temperature field which includes two hot spots which lag behind the center of the beam and are equidistant from the center line of the weld. In the case of small ring diameters these two hot spots can be close enough to the core beam that they can combine with it to create a wide capillary, the shape of which inhibits the formation of pores. When larger diameters are employed, the ring beam hot spots create a separate, secondary capillary (or capillaries) which may sporadically coalesce with the core beam capillary due to surface tension effects. When the capillaries merge, the depth of penetration of the combined capillary is reduced compared with the one created by the core alone. If the coalescence of the capillaries is sporadic then the weld stability is poor from both a porosity and a depth of penetration point of view.

Förderung

  • Universität Stuttgart

Zitieren

APA

Zaiß, F., Powell, J., Haas, M., Diegel, C., Schricker, K., Bergmann, J. P., Spurk, C., Hummel, M., Olowinsky, A., Beckmann, F., Moosmann, J., Hagenlocher, C., & Graf, T. (2026). X-Ray Imaging of Multi-Capillary Formation During Core-Ring Beam Laser Welding of Steel With Different Ring Beam Diameters. Lasers in Manufacturing and Materials Processing, 13(3), 677-698. https://doi.org/10.1007/s40516-026-00348-6

Vancouver

Zaiß F, Powell J, Haas M, Diegel C, Schricker K, Bergmann JP, et al. X-Ray Imaging of Multi-Capillary Formation During Core-Ring Beam Laser Welding of Steel With Different Ring Beam Diameters. Lasers in Manufacturing and Materials Processing. 2026;13(3):677-698. doi:10.1007/s40516-026-00348-6

BibTeX
@article{Zai2026,
  author = {Zaiß, Felix and Powell, John and Haas, Michael and Diegel, Christian and Schricker, Klaus and Bergmann, Jean Pierre and Spurk, Christoph and Hummel, Marc and Olowinsky, Alexander and Beckmann, Felix and Moosmann, Julian and Hagenlocher, Christian and Graf, Thomas},
  title = {X-Ray Imaging of Multi-Capillary Formation During Core-Ring Beam Laser Welding of Steel With Different Ring Beam Diameters},
  journal = {Lasers in Manufacturing and Materials Processing},
  year = {2026},
  volume = {13},
  number = {3},
  pages = {677--698},
  doi = {10.1007/s40516-026-00348-6}
}
Kostenlos starten →