Comparison of α-ferrite to ɣ-austenite transformations in 9%Cr steel alloys measured by neutron powder diffraction, dilatometry, and differential scanning calorimetry
Welding in the World · 22.05.2026
DOI: 10.1007/s40194-026-02485-0 ↗Kurz gefasst
Fachartikel in der Zeitschrift Welding in the World, online erschienen am 22.05.2026. Verfasst von Zeldah N. Sentsho und 4 weiteren Autor:innen. Die Arbeit nennt 49 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: University of Pretoria.
Abstract (Originalsprache)
This study explored phase transformations and thermal expansion coefficients in 9%Cr steels; P91 and P92 base metals, and P91 welds, on heating to 1000 °C. Neutron powder diffraction was employed to determine transformation temperatures, lattice parameters, and phase fractions. Austenite onset (A c1 ) and completion (A c3 ) temperatures were 800–805 °C and 885–890 °C for P91 base metal, and 814–816 °C and 928–930 °C for P92. The weld metals were evaluated in the as-welded condition. At room temperature, weld metals contained ferrite, martensite, and residual austenite. Residual austenite in weld 1 was retained on heating until fresh austenite formed at 765–770 °C, whereas in weld 2 it disappeared at 655–660 °C. The A c1 and A c3 temperatures of weld 2 were 815–820 °C and 920–922 °C. P92 transformed at lower temperatures and thermal expansion during the α-BCC-to-austenite transformation than P91. Weld 1 showed higher transformation temperatures and expansion than the base metal. Dilatometry measured transition temperatures of 817 °C and 880 °C for P91 base metal, and 836 °C and 923 °C for P92. As-welded curve exhibited multiple transitions between 697–904 °C. Calorimetry showed endothermic α-ferrite-to-austenite transitions with A c1 and A c3 at 824 °C and 874 °C for P91 base metal, 839 °C and 893 °C for P92, and 831 °C and 876 °C for weld 1. This study demonstrates the advantages of integrating neutron diffraction, dilatometry, and calorimetry to improve transformation analysis in 9%Cr steels; neutron diffraction measured A c1 up to 20 °C lower than dilatometry, indicating current post-weld heat treatment temperature ranges may be insufficiently conservative. Residual austenite in weld metal and its behaviour on heating may also influence weld heat-treatment response.
Förderung
- University of Pretoria
Zitieren
APA
Sentsho, Z. N., Pistorius, P. G. H., Venter, A. M., Hester, J. R., & Maynard-Casely, H. E. (2026). Comparison of α-ferrite to ɣ-austenite transformations in 9%Cr steel alloys measured by neutron powder diffraction, dilatometry, and differential scanning calorimetry. Welding in the World. https://doi.org/10.1007/s40194-026-02485-0
Vancouver
Sentsho ZN, Pistorius PGH, Venter AM, Hester JR, Maynard-Casely HE. Comparison of α-ferrite to ɣ-austenite transformations in 9%Cr steel alloys measured by neutron powder diffraction, dilatometry, and differential scanning calorimetry. Welding in the World. 2026. doi:10.1007/s40194-026-02485-0
BibTeX
@article{Sentsho2026,
author = {Sentsho, Zeldah N. and Pistorius, Pieter G. H. and Venter, Andrew M. and Hester, James R. and Maynard-Casely, Helen E.},
title = {Comparison of α-ferrite to ɣ-austenite transformations in 9%Cr steel alloys measured by neutron powder diffraction, dilatometry, and differential scanning calorimetry},
journal = {Welding in the World},
year = {2026},
doi = {10.1007/s40194-026-02485-0}
}
EUVIMED