Hydrogen Production Came from Catalytic Reforming of Volatiles Generated by Waste-Plastic Pyrolysis Over Sepiolite-Based Catalysts
Topics in Catalysis · 2025-01 · 68 (1-2) · 33-48
DOI: 10.1007/s11244-024-01981-1 ↗Kurz gefasst
Fachartikel in der Zeitschrift Topics in Catalysis, online erschienen am 27.06.2024. Verfasst von M. Ángeles Martín-Lara und 3 weiteren Autor:innen. Die Arbeit wurde bisher 14-mal zitiert (Crossref) und nennt 73 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Universidad de Granada.
Abstract (Originalsprache)
Several sepiolite-based catalysts have been prepared and investigated for pyrolytic H 2 production from a post-consumer mixture of residual plastics. The experimental installation involved a two-stage reaction system: first, the plastic mixture was thermally pyrolyzed at 500 ºC; then, the generated volatiles were reformed by increasing the temperature to 700 ºC and 800 ºC in the presence of the sepiolite-based catalysts. The real mixture came from non-separate waste collection streams and contained post-consumer polypropylene (rigid and film), expanded polystyrene, high-impact polystyrene, and polyethylene. The results demonstrated that the two-stage pyrolysis technique using sepiolite-based catalysts successfully generated hydrogen. The effects of the type of polymer, temperature, and catalyst were analyzed. The higher production of hydrogen (27.2 mmol H 2 /g) was obtained when the mixture of plastic waste was pyrolyzed and then the volatiles were reformed at 800 °C with the SN5-800 12 nickel-modified sepiolite. Additionally, the generation of hydrogen also increased after acidifying natural sepiolite (from 18.2 mmol H 2 /g plastic for natural sepiolite to 26.4 mmol H 2 /g for acidified sepiolite at 800 ºC with a plastic/catalyst ratio of 1:2). Finally, the carbon deposited in the catalysts was examined. Approximately, only 20% of the carbon that was deposited in the sepiolite-based catalysts was filamentous carbon; the majority was amorphous carbon. The results have therefore shown that it is possible to obtain a hydrogen-rich gas from the reforming of the pyrolysis vapors of a mixture of plastic waste using a low-cost catalyst based on nickel-modified sepiolite.
Förderung
- Universidad de Granada
Zitieren
APA
Martín-Lara, M. Á., Moreno, R., Blázquez, G., & Calero, M. (2025). Hydrogen Production Came from Catalytic Reforming of Volatiles Generated by Waste-Plastic Pyrolysis Over Sepiolite-Based Catalysts. Topics in Catalysis, 68(1-2), 33-48. https://doi.org/10.1007/s11244-024-01981-1
Vancouver
Martín-Lara MÁ, Moreno R, Blázquez G, Calero M. Hydrogen Production Came from Catalytic Reforming of Volatiles Generated by Waste-Plastic Pyrolysis Over Sepiolite-Based Catalysts. Topics in Catalysis. 2025;68(1-2):33-48. doi:10.1007/s11244-024-01981-1
BibTeX
@article{MartnLara2025,
author = {Martín-Lara, M. Ángeles and Moreno, R. and Blázquez, G. and Calero, M.},
title = {Hydrogen Production Came from Catalytic Reforming of Volatiles Generated by Waste-Plastic Pyrolysis Over Sepiolite-Based Catalysts},
journal = {Topics in Catalysis},
year = {2025},
volume = {68},
number = {1-2},
pages = {33--48},
doi = {10.1007/s11244-024-01981-1}
}
EUVIMED