Effect of different finishing/polishing protocols and aging on flexural strength, roughness, and surface characteristics of definitive restorative materials for CAD/CAM
Clinical Oral Investigations · 2026
DOI: 10.1007/s00784-026-07061-w ↗Kurz gefasst
Fachartikel in der Zeitschrift Clinical Oral Investigations, 2026. Verfasst von Helena Nóbrega Almeida und 7 weiteren Autor:innen. Beteiligte Einrichtung: Department of Dentistry, Federal University of Rio Grande do Norte (UFRN), Av. Salgado Filho. 1787. Lagoa Nova, Natal, RN, CEP: 59056-000, Brazil. Hauptthemen laut MEDLINE: Computer-Aided Design, Dental Polishing, Dental Materials. Die Arbeit nennt 44 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Universidade Federal Do Rio Grande Do Norte.
Abstract (Originalsprache)
Objective
To evaluate the effect of finishing/polishing and aging on the flexural strength, roughness, and surface characteristics of CAD/CAM restorative materials. Materials and methods Three CAD/CAM materials were tested: Nanoceramic resin (CR), Polymer-infiltrated ceramic (PIC), and Leucite-reinforced glass-ceramic (LC). A total of 120 bars (8 × 2 × 1 mm; n = 15/group) were prepared and subjected to different finishing/polishing protocols (C: control; B: bur; BD: diamond bur + diamond-impregnated rubber tips; BS: diamond bur + silica-impregnated rubbers) and aging (without/with 10,000 thermocycles). Mini-flexural strength (σ) was assessed by three-point bending. Surface roughness (Sa) was analyzed using optical profilometry, while surface characterization was performed using SEM. Data were analyzed with two-way ANOVA/Tukey’s test (α = 0.05) and Weibull analysis.
Results
For σ, both finishing/polishing and aging factors significantly affected PIC and LC ( p < 0.05), whereas only finishing/polishing influenced CR. In CR, aged CR_BD had the lowest strength (112.0 ± 17.9 MPa). In PIC, aged PIC_BS (121.8 ± 21.4) showed the highest strength, while PIC_BD groups showed the lowest. In LC, the highest values were seen in aged LC_C (125.7 ± 22.9), LC_B (114.75 ± 19.09), and non-aged LC_C (108.11 ± 29.54). Sa was significantly affected by material type and finishing/polishing protocols.
Conclusions
Silica-impregnated rubbers improved the flexural strength of PIC after bur finishing. The BD protocol, producing smoother surfaces, may compromise the flexural strength of LC. In contrast, CR was not significantly affected by the polishing protocol. Moreover, aging negatively impacted PIC strength, and polyurethane rubber tips impregnated with diamond particles produced smoother surfaces after bur adjustments. Clinical relevance Within the limitations of this in vitro study, polishing protocols should be selected according to material composition, since surface smoothness does not necessarily correlate with improved mechanical performance. For CR, all polishing systems showed comparable performance; for LC, minimal intervention or no polishing better preserved mechanical performance; for PIC, silica-based polishing systems may be preferred.
Schlagwörter
MeSH-Schlagwörter (MEDLINE)
Stichwörter der Autor:innen
Substanzen
Autor:innen und Institutionen
- Department of Dentistry, Federal University of Rio Grande do Norte (UFRN), Av. Salgado Filho. 1787. Lagoa Nova, Natal, RN, CEP: 59056-000, Brazil.
- Department of Dental Materials and Prosthodontics, Institute of Science and Technology, University Estadual Paulista - UNESP, Av. Eng. Francisco Jose Longo, 777, Sao Jose dos Campos, SP, 12245-000, Brazil.
- Department of Dentistry, Federal University of Rio Grande do Norte (UFRN), Av. Salgado Filho. 1787. Lagoa Nova, Natal, RN, CEP: 59056-000, Brazil. rodrigoothavio@gmail.com.
Förderung
- Universidade Federal Do Rio Grande Do Norte
Zitieren
APA
Almeida, H. N., de Oliveira, F. J. D., Santos, J. V. D. N., de Góis Moreira, F. G., Campos, B. O., de Melo, R. M., Borges, B. C. D., & de Assunção E Souza, R. O. (2026). Effect of different finishing/polishing protocols and aging on flexural strength, roughness, and surface characteristics of definitive restorative materials for CAD/CAM. Clinical Oral Investigations. https://doi.org/10.1007/s00784-026-07061-w
Vancouver
Almeida HN, de Oliveira FJD, Santos JVDN, de Góis Moreira FG, Campos BO, de Melo RM, et al. Effect of different finishing/polishing protocols and aging on flexural strength, roughness, and surface characteristics of definitive restorative materials for CAD/CAM. Clinical Oral Investigations. 2026. doi:10.1007/s00784-026-07061-w
BibTeX
@article{Almeida2026,
author = {Almeida, Helena Nóbrega and de Oliveira, Francisca Jennifer Duarte and Santos, João Vitor do Nascimento and de Góis Moreira, Fernanda Gurgel and Campos, Bruna Oliveira and de Melo, Renata Marques and Borges, Boniek Castillo Dutra and de Assunção E Souza, Rodrigo Othávio},
title = {Effect of different finishing/polishing protocols and aging on flexural strength, roughness, and surface characteristics of definitive restorative materials for CAD/CAM},
journal = {Clinical Oral Investigations},
year = {2026},
doi = {10.1007/s00784-026-07061-w}
}
EUVIMED