Effect of thermal aging on the radiopacity of universal composite resins at two thickness levels
Clinical Oral Investigations · 25.05.2026 · 30 (6)
DOI: 10.1007/s00784-026-06935-3 ↗Kurz gefasst
Fachartikel in der Zeitschrift Clinical Oral Investigations, online erschienen am 25.05.2026. Verfasst von Seyit Bilal Ozdemir und 1 weiteren Autor:innen. Beteiligte Einrichtung: Faculty of Dentistry Department of Restorative Dentistry, Giresun University, Goksuz Street & Number 15/17, Giresun, 28200, Turkey. Hauptthemen laut MEDLINE: Composite Resins. Die Arbeit wurde bisher 2-mal zitiert (Crossref) und nennt 39 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Giresun University.
Abstract (Originalsprache)
Objectives
The aim of this study was to investigate the effects of material type, specimen thickness, and thermocycling on the radiopacity of universal composite resins using equivalent aluminum thickness (mm Al). Materials and methods Four universal paste-type (Filtek Z250 Universal Restorative; FZ250, Omnichroma; OC, Vittra APS Unique; VU, and G-aenial Universal A’Chord; GU) and three universal flowable composite resins (Omnichroma Flow; OCF, Vittra APS Unique Flow; VUF, and G-aenial Universal Flo; GUF) were tested. Disk-shaped specimens (12 mm diameter) were prepared at 1 mm and 2 mm thicknesses ( n = 10 per group). Radiographic images were obtained using a digital X-ray system together with an aluminum step wedge and enamel–dentin references. Mean gray values (MGV) were measured using ImageJ software and converted to equivalent mm Al. Specimens were subjected to 10,000 thermocycles (5–55 °C). Data were analyzed using three-way ANOVA ( p < 0.05).
Results
Radiopacity differed significantly among the tested materials ( p < 0.001). FZ250 and VU exhibited the highest mm Al values at both thickness levels. Specimen thickness significantly affected radiopacity, with 2 mm specimens showing higher values than 1 mm specimens across all materials ( p < 0.001). After thermocycling, statistically significant decreases were observed in the 2 mm specimens of the VU and VUF groups ( p < 0.001). All materials exhibited radiopacity values equal to or greater than 1 mm Al at 1 mm thickness.
Conclusion
All tested universal composite resins met the minimum ISO 4049 radiopacity requirement. Radiopacity was influenced by material type and specimen thickness. Thermocycling caused a decrease in radiopacity values in some composite resin groups. Clinical relevance Thermocycling may affect radiopacity depending on material type and specimen thickness and should be considered by clinicians during radiographic evaluation of composite restorations.
Schlagwörter
MeSH-Schlagwörter (MEDLINE)
Stichwörter der Autor:innen
Substanzen
Autor:innen und Institutionen
- Faculty of Dentistry Department of Restorative Dentistry, Giresun University, Goksuz Street & Number 15/17, Giresun, 28200, Turkey.
- Faculty of Dentistry Department of Restorative Dentistry, Giresun University, Goksuz Street & Number 15/17, Giresun, 28200, Turkey. busrakbdy91@gmail.com.
Förderung
- Giresun University
Zitieren
APA
Ozdemir, S. B., & Ozdemir, B. (2026). Effect of thermal aging on the radiopacity of universal composite resins at two thickness levels. Clinical Oral Investigations, 30(6). https://doi.org/10.1007/s00784-026-06935-3
Vancouver
Ozdemir SB, Ozdemir B. Effect of thermal aging on the radiopacity of universal composite resins at two thickness levels. Clinical Oral Investigations. 2026;30(6). doi:10.1007/s00784-026-06935-3
BibTeX
@article{Ozdemir2026,
author = {Ozdemir, Seyit Bilal and Ozdemir, Busra},
title = {Effect of thermal aging on the radiopacity of universal composite resins at two thickness levels},
journal = {Clinical Oral Investigations},
year = {2026},
volume = {30},
number = {6},
doi = {10.1007/s00784-026-06935-3}
}
EUVIMED