Enhancement of zirconia–resin bonding by water glass surface treatment

Kota Kobayashi, Masaya Shimabukuro, Masaomi Ikeda, Kei Ushijima, Noriko Hiraishi, Masakazu Kawashita, Yasushi Shimada

Clinical Oral Investigations · 2026

DOI: 10.1007/s00784-026-06747-5 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Clinical Oral Investigations, 2026. Verfasst von Kota Kobayashi und 6 weiteren Autor:innen. Beteiligte Einrichtung: Department of Cariology and Operative Dentistry, Graduate School of Medical and Dental Sciences, Institute of Science Tokyo, 1-5-45, Yushima, Bunkyo-…. Hauptthemen laut MEDLINE: Zirconium, Dental Bonding, Composite Resins, Glass. Die Arbeit nennt 41 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY-NC-ND 4.0).

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

OBJECTIVES: This study evaluated the effect of water glass [(Na₂O)x(SiO₂)y] surface treatment on the bonding performance of zirconia to veneering porcelain and composite resin. Particular consideration was given to the clinical repair of fractured veneering porcelain on zirconia frameworks. MATERIALS AND METHODS: Zirconia specimens (5 mol% yttria-stabilized zirconia disk, 5Y-ZP) were divided into water-glass-treated and untreated groups, followed by sintering and alumina sandblasting (total n = 40; n = 10 per subgroup for resin testing). Surface roughness was analyzed by confocal laser microscopy, and elemental composition was examined using X-ray photoelectron spectroscopy (XPS). For porcelain testing, veneered specimens were subjected to shear bond strength (SBS) testing. For resin testing, specimens were bonded to composite resin with a silane-containing primer and divided into two subgroups: 24 h water storage at 37 °C and thermal cycling (5000 cycles, 5–55 °C). and then the SBS was measured. RESULTS: Water-glass treatment increased surface roughness and produced a silica-rich layer that persisted after sandblasting. Porcelain SBS was significantly higher in the treated group (29.5 ± 7.3 MPa) compared with the untreated group (15.2 ± 4.3 MPa, p < 0.05). For resin bonding, treated zirconia showed higher SBS under both 24 h (21.0 ± 2.3 vs. 15.6 ± 2.6 MPa) and thermal cycling (13.0 ± 2.4 vs. 7.1 ± 1.9 MPa) (p < 0.001). CONCLUSIONS: Water-glass treatment enhances resin–zirconia and porcelain–zirconia bonding by forming a durable silica-rich interface that resists sandblasting and promotes silane coupling. CLINICAL RELEVANCE: Water-glass pretreatment strengthens porcelain–zirconia adhesion and provides a stable surface for resin bonding, enabling reliable intraoral repair of porcelain-veneered zirconia crowns.

Schlagwörter

MeSH-Schlagwörter (MEDLINE)

ZirconiumDental BondingComposite ResinsGlassSurface PropertiesWaterMaterials TestingShear StrengthPhotoelectron SpectroscopyDental PorcelainMicroscopy, ConfocalDental VeneersAluminum Oxide

Stichwörter der Autor:innen

Resin bondingSilane couplingWater glassX-ray photoelectron spectroscopyZirconia

Substanzen

ZirconiumWaterComposite Resinszirconium oxideDental PorcelainAluminum Oxide

Autor:innen und Institutionen

  • Department of Cariology and Operative Dentistry, Graduate School of Medical and Dental Sciences, Institute of Science Tokyo, 1-5-45, Yushima, Bunkyo-ku, Tokyo, 113-8549, Japan.
  • Department of Inorganic Biomaterials, Laboratory for Biomaterials and Bioengineering, Institute of Integrated Research, Institute of Science Tokyo, Tokyo, Japan.
  • Department of Oral Biomedical Engineering, Graduate School of Medical and Dental Sciences, Institute of Science Tokyo, 1-5-45, Yushima, Bunkyo-ku, Tokyo, 113-8549, Japan. ikeda.csoe@tmd.ac.jp.
  • Department of Cariology and Operative Dentistry, Graduate School of Medical and Dental Sciences, Institute of Science Tokyo, 1-5-45, Yushima, Bunkyo-ku, Tokyo, 113-8549, Japan. hiraope@tmd.ac.jp.
  • Smart Innovations of Preventive and Restorative Dentistry Research Group, Department of Operative Dentistry, Faculty of Dentistry, Chulalongkorn University, Bangkok, Thailand. hiraope@tmd.ac.jp.

Zitieren

APA

Kobayashi, K., Shimabukuro, M., Ikeda, M., Ushijima, K., Hiraishi, N., Kawashita, M., & Shimada, Y. (2026). Enhancement of zirconia–resin bonding by water glass surface treatment. Clinical Oral Investigations. https://doi.org/10.1007/s00784-026-06747-5

Vancouver

Kobayashi K, Shimabukuro M, Ikeda M, Ushijima K, Hiraishi N, Kawashita M, et al. Enhancement of zirconia–resin bonding by water glass surface treatment. Clinical Oral Investigations. 2026. doi:10.1007/s00784-026-06747-5

BibTeX
@article{Kobayashi2026,
  author = {Kobayashi, Kota and Shimabukuro, Masaya and Ikeda, Masaomi and Ushijima, Kei and Hiraishi, Noriko and Kawashita, Masakazu and Shimada, Yasushi},
  title = {Enhancement of zirconia–resin bonding by water glass surface treatment},
  journal = {Clinical Oral Investigations},
  year = {2026},
  doi = {10.1007/s00784-026-06747-5}
}
Kostenlos starten →