Kinetics and mechanisms of high-temperature oxidation of stainless steel 347LSi in synthetic air

Gleryston T. G. da Silva, Helen R. Araújo, André A. Vicente, Aureliano X. Santos, Renato A. C. de Santana, Edwar A. Torres-López, Tiago Felipe A. Santos

The International Journal of Advanced Manufacturing Technology · 04.11.2026

DOI: 10.1007/s00170-026-19406-6 ↗

Kurz gefasst

Fachartikel in der Zeitschrift The International Journal of Advanced Manufacturing Technology, online erschienen am 04.11.2026. Verfasst von Gleryston T. G. da Silva und 6 weiteren Autor:innen. Die Arbeit nennt 45 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Universidade Federal De Pernambuco.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

The high-temperature oxidation behavior of 347LSi stainless steel coatings is a critical factor for their application in aggressive environments. This study investigates the oxidation kinetics and mechanisms of coatings deposited by GMAW process on 2.25Cr–1Mo steel substrates, using different Ar–CO 2 shielding gas mixtures, in a synthetic air atmosphere at 800, 900, 1000, and 1100 °C. Thermogravimetric analysis revealed predominantly parabolic oxidation behavior for all conditions at times above 10 4 s, allowing the determination of parabolic rate constants (kₚ) and apparent activation energies (Eₐ). At 800 °C, the coatings exhibited low kₚ values and formed a compact and adherent bilayer oxide scale composed of an inner Cr 2 O 3 layer and an outer (Fe, Mn, Cr) 2 O 4 spinel, providing effective protection against oxidation. As the temperature increased to 900–1100 °C, a transition to accelerated oxidation was observed, associated with chromium depletion at the metal/oxide interface and the progressive breakdown of the protective chromia layer. This resulted in the formation of Fe-rich, porous, and poorly adherent oxides, promoting oxide spallation and loss of protective behavior. The shielding gas composition significantly influenced oxidation performance. The mixture containing 4% CO 2 exhibited the best overall behavior, combining lower oxidation rates with improved oxide stability, whereas higher CO 2 contents promoted faster degradation at elevated temperatures. These results demonstrate that oxidation resistance is maintained up to approximately 800 °C, while higher temperatures lead to a transition toward non-protective oxidation mechanisms. The findings highlight the critical role of shielding gas selection in controlling high-temperature oxidation and provide practical guidelines for the design of stainless steel coatings for demanding service conditions.

Förderung

  • Universidade Federal De Pernambuco

Zitieren

APA

Silva, G. T. G. D., Araújo, H. R., Vicente, A. A., Santos, A. X., Santana, R. A. C. D., Torres-López, E. A., & Santos, T. F. A. (2026). Kinetics and mechanisms of high-temperature oxidation of stainless steel 347LSi in synthetic air. The International Journal of Advanced Manufacturing Technology. https://doi.org/10.1007/s00170-026-19406-6

Vancouver

Silva GTGD, Araújo HR, Vicente AA, Santos AX, Santana RACD, Torres-López EA, et al. Kinetics and mechanisms of high-temperature oxidation of stainless steel 347LSi in synthetic air. The International Journal of Advanced Manufacturing Technology. 2026. doi:10.1007/s00170-026-19406-6

BibTeX
@article{Silva2026,
  author = {Silva, Gleryston T. G. da and Araújo, Helen R. and Vicente, André A. and Santos, Aureliano X. and Santana, Renato A. C. de and Torres-López, Edwar A. and Santos, Tiago Felipe A.},
  title = {Kinetics and mechanisms of high-temperature oxidation of stainless steel 347LSi in synthetic air},
  journal = {The International Journal of Advanced Manufacturing Technology},
  year = {2026},
  doi = {10.1007/s00170-026-19406-6}
}
Kostenlos starten →