Mitigating Mn‐Driven Interfacial Instability in LiMn 0.5 Fe 0.5 PO 4 Cathodes for Lithium‐Ion Batteries via Surface‐Intensive Ta Doping
Small · 2026-05 · 22 (29)
DOI: 10.1002/smll.73307 ↗Kurz gefasst
Fachartikel in der Zeitschrift Small, online erschienen am 03.04.2026. Verfasst von Hyeji Lee und 3 weiteren Autor:innen. Beteiligte Einrichtung: Department of Energy Engineering, Konkuk University, Seoul, Republic of Korea. Die Arbeit wurde bisher 2-mal zitiert (Crossref) und nennt 68 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY-NC-ND 4.0). Gefördert von: National Research Foundation of Korea, Korea government.
Abstract (Originalsprache)
LiMn x Fe 1−x PO 4 (LMFP) holds promise for next‐generation olivine‐type cathodes for Li‐ion batteries but suffers from sluggish Li + diffusion along 1D [010] channels. Moreover, because Jahn‐Teller‐active Mn 3+ species are involved, LMFP exhibits increased polarization and progressive performance degradation under high‐rate and low‐temperature conditions. Consequently, the Mn 2+ /Mn 3+ redox becomes surface‐intensive at the near‐surface region, thereby triggering Mn dissolution and electrolyte side reactions. To address this problem, we use surface‐intensive Ta doping, exploiting the slow diffusion kinetics of Ta 5+ to selectively enrich the near‐surface region of LiMn 0.5 Fe 0.5 PO 4 particles in Ta. Ta doping strengthens the M─O framework and widens the Li─O diffusion pathways while increasing the near‐surface Mn 2+ fraction from 53.9% to 59.7%, thereby suppressing Mn 3+ accumulation. Electrochemically, Ta1@LMFP delivers 105.58 mAh g −1 at 20 C (71.1% of the 0.1 C capacity), outperforming Ta0@LMFP (82.27 mAh g −1 , 54.8%). In addition, under high‐SOC storage conditions (60°C, 10d), Ta1@LMFP maintains 99.5% of its initial capacity, whereas Ta0@LMFP retains 83.1%, confirming that self‐discharge and interfacial degradation are suppressed at high temperature and high SOC. This work demonstrates that surface‐intensive Ta doping enables the wide‐temperature‐range and high‐power operation of LMFP‐based cathodes and provides compositional and structural design guidelines for developing robust cathode materials for Li‐ion batteries.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- Department of Energy Engineering, Konkuk University, Seoul, Republic of Korea.
- Department of Materials Science and Engineering, Konkuk University, Seoul, Republic of Korea.
- Advanced Materials Programs, Department of Materials Science and Engineering, Konkuk University, Seoul, Republic of Korea.
ORCID-Profile: Ji-Won Jung, Wonchang Choi
Förderung
- National Research Foundation of Korea
- Korea government
Zitieren
APA
Lee, H., Lee, W., Jung, J. W., & Choi, W. (2026). Mitigating Mn‐Driven Interfacial Instability in LiMn 0.5 Fe 0.5 PO 4 Cathodes for Lithium‐Ion Batteries via Surface‐Intensive Ta Doping. Small, 22(29). https://doi.org/10.1002/smll.73307
Vancouver
Lee H, Lee W, Jung JW, Choi W. Mitigating Mn‐Driven Interfacial Instability in LiMn 0.5 Fe 0.5 PO 4 Cathodes for Lithium‐Ion Batteries via Surface‐Intensive Ta Doping. Small. 2026;22(29). doi:10.1002/smll.73307
BibTeX
@article{Lee2026,
author = {Lee, Hyeji and Lee, Wonjun and Jung, Ji-Won and Choi, Wonchang},
title = {Mitigating Mn‐Driven Interfacial Instability in LiMn 0.5 Fe 0.5 PO 4 Cathodes for Lithium‐Ion Batteries via Surface‐Intensive Ta Doping},
journal = {Small},
year = {2026},
volume = {22},
number = {29},
doi = {10.1002/smll.73307}
}
EUVIMED