EUVIMEDEUVIMED entdecken
Crossref

Optimizing the Imidazolium Cation Alkyl Chain Length in Water‐in‐Ionic Liquid Electrolytes for Enhanced Interfacial Stability in Aqueous Zinc‐Ion Batteries

Eunha Seo, Juyeon Han, Jeeyoung Yoo iD

Small · 2026-02 · 22 (7)

DOI: 10.1002/smll.202511769 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Small, online erschienen am 09.12.2025. Verfasst von Eunha Seo und 2 weiteren Autor:innen. Beteiligte Einrichtung: School of Energy Engineering, Kyungpook National University, Daegu, 41566, Republic of Korea. Die Arbeit wurde bisher 1-mal zitiert (Crossref) und nennt 53 Literaturangaben. Gefördert von: National Research Foundation of Korea.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Aqueous Zn‐ion batteries (AZIBs) show promise for large‐scale energy‐storage applications due to Zn being Earth‐abundant and their stability. Nevertheless, the translational viability of these systems is curtailed by nonuniform Zn electrodeposition, particularly dendritic growth, and by multiple parasitic reactions occurring at the Zn | electrolyte interphase. To resolve these issues, hybrid electrolytes are prepared by first making a 2 m Zn(OTf) 2 aqueous solution, which is subsequently mixed with imidazolium‐based ionic liquids—1‐ethyl‐3‐methylimidazolium (EMIm), 1‐butyl‐3‐methylimidazolium (BMIm), and 1‐hexyl‐3‐methylimidazolium (HMIm)—at a 1:1 (v/v) ratio. After mixing, the final hybrid electrolyte contained 1 m Zn(OTf) 2 . Short alkyl chain length EMIm⁺ is preferentially adsorbed onto the Zn(100) and Zn(101) facets, thereby suppressing needle‐like dendrite formation and promoting uniform Zn deposition, whereas an OTf‐derived inorganic‐organic composite solid electrolyte interphase mitigates parasitic interfacial reactions. Consequently, an ammonium vanadate nanofiber∥Zn half‐cell retains 82% of its initial capacity after 3600 cycles at 2 A g −1 , while an EMIm‐based Zn∥Zn symmetric cell operates stably for more than 830 h at 1 mA cm −2 , thereby corroborating the electrolyte's interfacial robustness. This study reveals that choosing the appropriate alkyl chain length of the imidazole cation in a hybrid electrolyte enables highly reversible Zn chemistry and long‐term cycling stability in AZIBs.

Schlagwörter

Stichwörter der Autor:innen

aqueous zinc‐ion batteryhybrid electrolyteimidazoliumionic liquid

Autor:innen und Institutionen

  • School of Energy Engineering, Kyungpook National University, Daegu, 41566, Republic of Korea.

ORCID-Profile: Jeeyoung Yoo

Förderung

  • National Research Foundation of Korea

Zitieren

APA

Seo, E., Han, J., & Yoo, J. (2026). Optimizing the Imidazolium Cation Alkyl Chain Length in Water‐in‐Ionic Liquid Electrolytes for Enhanced Interfacial Stability in Aqueous Zinc‐Ion Batteries. Small, 22(7). https://doi.org/10.1002/smll.202511769

Vancouver

Seo E, Han J, Yoo J. Optimizing the Imidazolium Cation Alkyl Chain Length in Water‐in‐Ionic Liquid Electrolytes for Enhanced Interfacial Stability in Aqueous Zinc‐Ion Batteries. Small. 2026;22(7). doi:10.1002/smll.202511769

BibTeX
@article{Seo2026,
  author = {Seo, Eunha and Han, Juyeon and Yoo, Jeeyoung},
  title = {Optimizing the Imidazolium Cation Alkyl Chain Length in Water‐in‐Ionic Liquid Electrolytes for Enhanced Interfacial Stability in Aqueous Zinc‐Ion Batteries},
  journal = {Small},
  year = {2026},
  volume = {22},
  number = {7},
  doi = {10.1002/smll.202511769}
}
Kostenlos starten →