Charge‐Induced Defective MOF‐801 with Enhanced Sorption Heat for Efficient Hydrogen Storage

Jia Chen, Zhuozhuo Tang, Da Zhu, Li Sheng, Yang Yang, Jianlong Wang, Yaping Tang, Xiangming He, Hong Xu iD

Small · 2025-06 · 21 (23)

DOI: 10.1002/smll.202502860 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Small, online erschienen am 18.04.2025. Verfasst von Jia Chen und 8 weiteren Autor:innen. Beteiligte Einrichtung: Institute of Nuclear and New Energy Technology, Tsinghua University, Beijing, 100084, China. Die Arbeit wurde bisher 11-mal zitiert (Crossref) und nennt 55 Literaturangaben. Gefördert von: National Natural Science Foundation of China, Ministry of Science and Technology of China, Tsinghua Initiative Scientific Research Program.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Metal–organic frameworks (MOFs) are considered ideal candidates for H 2 physisorption materials due to their high surface area and tunable pore structures/environments. However, their interaction with hydrogen is too weak to fully exploit their surface area advantages, necessitating the exploration of effective adsorption enhancement strategies. Here, a defective MOF‐801 is reported as an H 2 physisorption material and investigate the enhancement of hydrogen adsorption by charge‐inducing. Based on the excellent stability of MOF‐801, the material retains good porosity after acid vapor etching, compared to the initial MOF‐801 (810 m 2 g −1 ), the surface area reaching up to 970 m 2 g −1 . The mild etching method leads to excess charges around the zirconium (Zr) of MOF‐801, forming specific defective sites with excellent adsorption heat, inducing hydrogen polarization, and enhancing hydrogen capacity. The total H 2 uptake increases from 5.02 wt.% (MOF‐801) to 8.58 wt.% (Cl@MOF‐801) at 77 K and 80 bar. Additionally, the material exhibits excellent cycling performance, stably cycling 10 times at 8 MPa and maintaining a total capacity of 8.56 wt%. The results reveal that tuning H 2 adsorption heat by charge induction is a promising strategy to exploit the potential of porous materials for efficient H 2 storage.

Schlagwörter

Stichwörter der Autor:innen

acid vapor etchingcharge inductiondefective MOF‐801hydrogen storagesorption heat

Autor:innen und Institutionen

  • Institute of Nuclear and New Energy Technology, Tsinghua University, Beijing, 100084, China.

ORCID-Profile: Hong Xu

Förderung

  • National Natural Science Foundation of China
  • Ministry of Science and Technology of China
  • Tsinghua Initiative Scientific Research Program
  • Ministry of Science and Technology of the People's Republic of China

Zitieren

APA

Chen, J., Tang, Z., Zhu, D., Sheng, L., Yang, Y., Wang, J., Tang, Y., He, X., & Xu, H. (2025). Charge‐Induced Defective MOF‐801 with Enhanced Sorption Heat for Efficient Hydrogen Storage. Small, 21(23). https://doi.org/10.1002/smll.202502860

Vancouver

Chen J, Tang Z, Zhu D, Sheng L, Yang Y, Wang J, et al. Charge‐Induced Defective MOF‐801 with Enhanced Sorption Heat for Efficient Hydrogen Storage. Small. 2025;21(23). doi:10.1002/smll.202502860

BibTeX
@article{Chen2025,
  author = {Chen, Jia and Tang, Zhuozhuo and Zhu, Da and Sheng, Li and Yang, Yang and Wang, Jianlong and Tang, Yaping and He, Xiangming and Xu, Hong},
  title = {Charge‐Induced Defective MOF‐801 with Enhanced Sorption Heat for Efficient Hydrogen Storage},
  journal = {Small},
  year = {2025},
  volume = {21},
  number = {23},
  doi = {10.1002/smll.202502860}
}
Kostenlos starten →