Fachartikel in der Zeitschrift Small, online erschienen am 17.04.2025. Verfasst von Ge Qu und 10 weiteren Autor:innen. Beteiligte Einrichtung: School of Materials Science and Engineering, Tongji University, Shanghai, 201804, China. Die Arbeit wurde bisher 10-mal zitiert (Crossref) und nennt 48 Literaturangaben. Gefördert von: Key Technologies Research and Development Program, Fundamental Research Funds for Central Universities.
Abstract (Originalsprache)
Nickel‐rich layered cathodes are promising for high‐energy‐density lithium‐ion batteries but suffer from rapid capacity fading, primarily due to intergranular cracking and structural degradation during the H2‐H3 phase transition, especially under high voltage. To address these challenges, a novel Ta 5+ /Ti 4+ co‐doping strategy has been introduced that simultaneously stabilizes grain boundaries and enhances the mechanical strength of the cathode. The dopants effectively mitigate intergranular cracking and form a pre‐cation‐mixing layer, stabilizing the layered structure during deep delithiation and preventing structural collapse. Moreover, this co‐doping approach also improves the reversibility of the H2‐H3 phase transition and reduces lattice distortions, thereby enhancing cycling stability. As a result, the co‐doped cathode exhibits excellent capacity retention of 96.66% after 150 cycles at 1 C in liquid electrolyte. In solid‐state batteries, it demonstrates superior interfacial compatibility with significantly reduced side reactions with the solid electrolyte, achieving a high initial capacity of 181.4 mAh g −1 and retaining 89.3% of its capacity after 100 cycles. This marks a significant improvement over the pristine cathode. These results highlight the effectiveness of Ta 5+ /Ti 4+ co‐doping as a pratical strategy for developing high‐performance nickel‐rich cathodes for next‐generation lithium‐ion batteries.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- School of Materials Science and Engineering, Tongji University, Shanghai, 201804, China.
- Department of Mining and Materials Engineering, McGill University, Montréal, QC, H3A 0C5, Canada.
- Institute of Chemistry, Chinese Academy of Sciences, Beijing, 100190, China.
- State Key Laboratory of Material Processing and Die & Mould Technology, School of Materials Science and Engineering, Huazhong University of Science and Technology, Wuhan, Hubei, 430074, China.
ORCID-Profile: Ge Qu, Yunhui Huang
Förderung
- Key Technologies Research and Development Program
- Fundamental Research Funds for Central Universities
Zitieren
APA
Qu, G., Chen, X., Yang, F., Yang, Z., Liu, G., Lee, J., Fong, R., Tian, J., Wen, R., Wang, C., & Huang, Y. (2025). Boosting Ni‐Rich Cathode Stability Through Grain Boundary Strengthening and Phase Transition Degradation Suppression. Small, 21(23). https://doi.org/10.1002/smll.202502609
Vancouver
Qu G, Chen X, Yang F, Yang Z, Liu G, Lee J, et al. Boosting Ni‐Rich Cathode Stability Through Grain Boundary Strengthening and Phase Transition Degradation Suppression. Small. 2025;21(23). doi:10.1002/smll.202502609
BibTeX
@article{Qu2025,
author = {Qu, Ge and Chen, Xinlong and Yang, Fangzhou and Yang, Zhiqi and Liu, Ganxiong and Lee, Jinhyuk and Fong, Richie and Tian, Jianxin and Wen, Rui and Wang, Chao and Huang, Yunhui},
title = {Boosting Ni‐Rich Cathode Stability Through Grain Boundary Strengthening and Phase Transition Degradation Suppression},
journal = {Small},
year = {2025},
volume = {21},
number = {23},
doi = {10.1002/smll.202502609}
}
EUVIMED