EUVIMEDEUVIMED entdecken
Crossref

Sharply Improved Electrical Insulation of Polyimide Dielectrics at Elevated Temperatures by Charge Reassignment Engineering

Chuanfang Yan, Jinlong Zhou, Ao Xu, Hongping Long, Hang Luo, Sheng Chen iD

Small · 2025-06 · 21 (24)

DOI: 10.1002/smll.202501050 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Small, online erschienen am 22.04.2025. Verfasst von Chuanfang Yan und 5 weiteren Autor:innen. Beteiligte Einrichtung: Key Laboratory of Polymeric Materials and Application Technology of Hunan Province, College of Chemistry, Xiangtan University, Xiangtan, Hunan, 41110…. Die Arbeit wurde bisher 18-mal zitiert (Crossref) und nennt 64 Literaturangaben. Gefördert von: Scientific Research Fund of the Hunan Provincial Education Department, Excellent Youth Science Foundation of Hunan Province.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

The electrical insulation of traditional polyimides (PI) dielectrics for capacitive energy storage will be significantly destroyed at elevated temperatures due to enhanced conductive loss caused by strong conjugated effect and charge transfer (CT) interactions. To address this issue, novel PI dielectrics are designed and synthesized based on charge reassignment engineering. Beneficial from non‐planar dianhydride and poor conjugated diamine, the main chain of synthesized PI (semi‐aromatic NA 2 ‐ alt ‐OB 1 ) significantly reduces the conjugated effect. Alicyclic dianhydride structural unit endows NA 2 ‐ alt ‐OB 1 with a large bandgap width of 5.22 eV and a high LUMO energy level (−0.79 eV), making the polymer resistant to both excited and injected electrons. More importantly, this work intelligently combines trifluoromethyl and dicyclohexyl to achieve weak charge reassignment on donor–acceptor electron sites in the polymer chain, effectively decreasing CT effect. Consequently, a super‐high Weibull breakdown strength value of 862 and 691 MV m −1 at room temperature and 230 °C respectively is achieved. Semi‐aromatic NA 2 ‐ alt ‐OB 1 obtains a high discharge energy density of 6.43 J cm −3 at 230 °C, which is greater than that of lots of reported PI dielectrics. This work offers an important strategy to break the adverse correlation between electrical insulation and heating resistance of PI dielectrics, promoting their application in capacitive energy storage at elevated temperatures.

Schlagwörter

Stichwörter der Autor:innen

energy storageinsulating propertypolyimideultrahigh temperature

Autor:innen und Institutionen

  • Key Laboratory of Polymeric Materials and Application Technology of Hunan Province, College of Chemistry, Xiangtan University, Xiangtan, Hunan, 411105, China.
  • State Key Laboratory of Powder Metallurgy, Central South University, Changsha, Hunan, 410083, China.

ORCID-Profile: Sheng Chen

Förderung

  • Scientific Research Fund of the Hunan Provincial Education Department
  • Excellent Youth Science Foundation of Hunan Province

Zitieren

APA

Yan, C., Zhou, J., Xu, A., Long, H., Luo, H., & Chen, S. (2025). Sharply Improved Electrical Insulation of Polyimide Dielectrics at Elevated Temperatures by Charge Reassignment Engineering. Small, 21(24). https://doi.org/10.1002/smll.202501050

Vancouver

Yan C, Zhou J, Xu A, Long H, Luo H, Chen S. Sharply Improved Electrical Insulation of Polyimide Dielectrics at Elevated Temperatures by Charge Reassignment Engineering. Small. 2025;21(24). doi:10.1002/smll.202501050

BibTeX
@article{Yan2025,
  author = {Yan, Chuanfang and Zhou, Jinlong and Xu, Ao and Long, Hongping and Luo, Hang and Chen, Sheng},
  title = {Sharply Improved Electrical Insulation of Polyimide Dielectrics at Elevated Temperatures by Charge Reassignment Engineering},
  journal = {Small},
  year = {2025},
  volume = {21},
  number = {24},
  doi = {10.1002/smll.202501050}
}
Kostenlos starten →