Ferroelectric Interfaces for Dendrite Prevention in Zinc‐Ion Batteries

Xueqing Hu, Bastola Narayan, Nibagani Naresh, Iman Pinnock, Yijia Zhu, Xiaopeng Liu, Tianlei Wang, Bing Li, Ivan P Parkin, Buddha Deka Boruah iD

Small · 2024-12 · 20 (49)

DOI: 10.1002/smll.202403555 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Small, online erschienen am 15.09.2024. Verfasst von Xueqing Hu und 9 weiteren Autor:innen. Beteiligte Einrichtung: Institute for Materials Discovery (IMD), University College London (UCL), London, WC1E 7JE, UK. Die Arbeit wurde bisher 18-mal zitiert (Crossref) und nennt 21 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Aqueous rechargeable zinc‐ion batteries (ZIBs) are increasingly recognized as promising energy storage systems for mini‐grid and mini‐off‐grid applications due to their advantageous characteristics such as high safety, affordability, and considerable theoretical capacity. However, the long‐term cycling performance of ZIBs is hampered by challenges including the uncontrolled dendrite formation, the passivation, and the occurrence of the hydrogen evolution reaction (HER) on the Zn anode. In this study, enhancing ZIB performance by implementing oxide material coatings on Zn metal, serving as a physical barrier at the electrode‐electrolyte interfaces to mitigate dendrite growth and suppress the HER is concentrated. Specifically, the mechanisms through which the n‐type semiconductor TiO 2 coated Zn anode establishes ohmic contact with Zn, and the high‐dielectric BaTiO 3 (BTO) coated Zn anode fosters Maxwell‐Wagner polarization with ferroelectric properties, significantly inhibiting dendrite growth and side reactions, thereby resulting in a highly stable Zn anode for efficient aqueous ZIBs is explored. This advanced BTO/Zn electrode demonstrates an extended lifespan of over 700 h compared to bare Zn and TiO 2 /Zn anodes. Additionally, full‐cell aqueous ZIBs incorporating BTO/Zn//VO 2 (B) batteries exhibit superior rate capabilities, high capacity, and sustained cycle life.

Schlagwörter

Stichwörter der Autor:innen

dendrite suppressionferroelectricohmic contactzn anodeszn‐ion batteries

Autor:innen und Institutionen

  • Institute for Materials Discovery (IMD), University College London (UCL), London, WC1E 7JE, UK.
  • Department of Mechanical Engineering, University of Bath, Bath, BA2 7AY, UK.
  • Department of Chemistry, University College London (UCL), London, WC1H 0AJ, UK.

ORCID-Profile: Buddha Deka Boruah

Zitieren

APA

Hu, X., Narayan, B., Naresh, N., Pinnock, I., Zhu, Y., Liu, X., Wang, T., Li, B., Parkin, I. P., & Boruah, B. D. (2024). Ferroelectric Interfaces for Dendrite Prevention in Zinc‐Ion Batteries. Small, 20(49). https://doi.org/10.1002/smll.202403555

Vancouver

Hu X, Narayan B, Naresh N, Pinnock I, Zhu Y, Liu X, et al. Ferroelectric Interfaces for Dendrite Prevention in Zinc‐Ion Batteries. Small. 2024;20(49). doi:10.1002/smll.202403555

BibTeX
@article{Hu2024,
  author = {Hu, Xueqing and Narayan, Bastola and Naresh, Nibagani and Pinnock, Iman and Zhu, Yijia and Liu, Xiaopeng and Wang, Tianlei and Li, Bing and Parkin, Ivan P and Boruah, Buddha Deka},
  title = {Ferroelectric Interfaces for Dendrite Prevention in Zinc‐Ion Batteries},
  journal = {Small},
  year = {2024},
  volume = {20},
  number = {49},
  doi = {10.1002/smll.202403555}
}
Kostenlos starten →