Modified bismaleimide with benzoxazine containing tert ‐butyl group: preparation, characterization and properties
Polymer International · 18.11.2026
DOI: 10.1002/pi.70224 ↗Kurz gefasst
Fachartikel in der Zeitschrift Polymer International, online erschienen am 18.11.2026. Verfasst von Yiqing Xia und 10 weiteren Autor:innen. Die Arbeit nennt 43 Literaturangaben. Gefördert von: Sichuan Provincial Science and Technology Support Program.
Abstract (Originalsprache)
With the rapid development of high‐frequency communication and electronic integrated circuits, high thermal performance and low dielectric resin have become active research areas in recent years. In this paper, four benzoxazines (Bz, Bz‐o, Bz‐p, Bz‐m) were synthesized by Mannich reaction of trimethylhexanediamine, paraformaldehyde and different phenols (phenol, o ‐ tert ‐butylphenol, m ‐ tert ‐butylphenol and p ‐ tert ‐butylphenol). The chemical structure and curing behavior of the benzoxazine monomers were characterized using Fourier transform infrared and 1 H NMR spectroscopies and differential scanning calorimetry, and the results showed that four benzoxazine resins were successfully synthesized. And then, these benzoxazines were used to modify bismaleimide resin (BMI‐70) by copolymerization, and the effects of introduction of the tert ‐butyl group and its substitution position on properties were explored. The results demonstrated that incorporating the low‐polarity, bulky tert ‐butyl group reduced the polarizability of the copolymers and increased their free volume, thereby improving their dielectric properties. The dielectric constant ( D k ) of the copolymer decreased from 3.09 to 2.87 at 10 MHz, while the dissipation factor ( D f ) ranged from 0.0024 to 0.0041 at 10 MHz. Water absorption was also markedly reduced: the tert ‐butyl‐containing copolymers absorbed 2.06–2.47% water, compared with 3.02% for P(BMI/Bz). Among these prepared copolymers, the para ‐substituted tert ‐butyl variant exhibited the most balanced overall performance, with a glass transition temperature of 298 °C, D k of 2.88, D f of 0.0026, water absorption of 2.43% and CY of 33.4% at 800 °C. These results confirm that introducing the tert ‐butyl group effectively improves the dielectric properties, thermal stability and moisture resistance of benzoxazine‐modified BMI systems, suggesting that these copolymers are promising low‐dielectric thermoset candidates. © 2026 Society of Chemical Industry.
Förderung
- Sichuan Provincial Science and Technology Support Program
Zitieren
APA
Xia, Y., Zhou, Z., Sheng, Y., Yan, S., Zhu, C., Emori, W., Zhang, R., Fu, C., Cai, W., Zhang, Y., & Wang, Q. (2026). Modified bismaleimide with benzoxazine containing tert ‐butyl group: preparation, characterization and properties. Polymer International. https://doi.org/10.1002/pi.70224
Vancouver
Xia Y, Zhou Z, Sheng Y, Yan S, Zhu C, Emori W, et al. Modified bismaleimide with benzoxazine containing tert ‐butyl group: preparation, characterization and properties. Polymer International. 2026. doi:10.1002/pi.70224
BibTeX
@article{Xia2026,
author = {Xia, Yiqing and Zhou, Zhenggang and Sheng, Yuping and Yan, Shuai and Zhu, Chunguang and Emori, Wilfred and Zhang, Renfei and Fu, Chenghong and Cai, Wei and Zhang, Youwen and Wang, Qiushi},
title = {Modified bismaleimide with benzoxazine containing tert ‐butyl group: preparation, characterization and properties},
journal = {Polymer International},
year = {2026},
doi = {10.1002/pi.70224}
}
EUVIMED