Wrinkled thermoplastic polyamide elastomer foams with enhanced mechanical properties fabricated by dynamic supercritical CO 2 foaming

Weipeng Zhong, Xu Zhou, Miaomiao Zhang, Wenhao Cui, Hao‐Yang Mi, Binbin Dong, Chuntai Liu, Changyu Shen

Polymer Engineering & Science · 2025-02 · 65 (2) · 834-845

DOI: 10.1002/pen.27048 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Polymer Engineering & Science, online erschienen am 31.12.2024. Verfasst von Weipeng Zhong und 7 weiteren Autor:innen. Die Arbeit wurde bisher 4-mal zitiert (Crossref) und nennt 56 Literaturangaben. Gefördert von: National Natural Science Foundation of China.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Wrinkled foams (WF), distinguished by their numerous cell wall wrinkles, exhibit superior impact resistance compared to conventional foams (CF), making them ideal for applications such as sports protection and packaging. Despite their potential, the mechanisms behind wrinkle formation remain underexplored, limiting production and process optimization. In this study, we use a custom supercritical foaming reactor with a sapphire glass viewing window to investigate the differences between wrinkled and conventional thermoplastic polyamide elastomer foams. Our findings suggest that “excessive expansion‐shrinkage” is crucial for wrinkle development. Molecular dynamics simulations reveal that molecular chains align with the flow field of dynamic CO 2 , which increases the intramolecular stress. The release of intramolecular stress triggers wrinkle formation, driven by thermodynamic instability. Furthermore, comparisons of the impact resistance and compression performance between WF and CF show that wrinkled structures alter the deformation behavior under force. The wrinkles facilitate increased collision, squeezing, and friction between cell walls, thus dissipating energy as heat and creating “micro‐air units” that enhance cushioning capability. These distinctive characteristics make WF a promising material for high‐performance applications in cushioning and energy absorption, such as in sports protection and packaging. Highlights Wrinkled polyamide foams are fabricated by dynamic scCO 2 foaming. Chain stretching and shrinkage under scCO 2 flow are verified by MD simulation. Excessive expansion‐shrinkage foaming behavior causes the wrinkled structure. Wrinkled structure greatly increases the impact absorption ability.

Förderung

  • National Natural Science Foundation of China

Zitieren

APA

Zhong, W., Zhou, X., Zhang, M., Cui, W., Mi, H., Dong, B., Liu, C., & Shen, C. (2025). Wrinkled thermoplastic polyamide elastomer foams with enhanced mechanical properties fabricated by dynamic supercritical CO 2 foaming. Polymer Engineering & Science, 65(2), 834-845. https://doi.org/10.1002/pen.27048

Vancouver

Zhong W, Zhou X, Zhang M, Cui W, Mi H, Dong B, et al. Wrinkled thermoplastic polyamide elastomer foams with enhanced mechanical properties fabricated by dynamic supercritical CO 2 foaming. Polymer Engineering & Science. 2025;65(2):834-845. doi:10.1002/pen.27048

BibTeX
@article{Zhong2025,
  author = {Zhong, Weipeng and Zhou, Xu and Zhang, Miaomiao and Cui, Wenhao and Mi, Hao‐Yang and Dong, Binbin and Liu, Chuntai and Shen, Changyu},
  title = {Wrinkled thermoplastic polyamide elastomer foams with enhanced mechanical properties fabricated by dynamic supercritical CO 2 foaming},
  journal = {Polymer Engineering & Science},
  year = {2025},
  volume = {65},
  number = {2},
  pages = {834--845},
  doi = {10.1002/pen.27048}
}
Kostenlos starten →