EUVIMEDEUVIMED entdecken
Crossref

Renewable thermoplastic starch/sugar alcohol blends and their oxygen barrier application

Hong‐juan Xu, Han‐fang Mei, Wei‐xing Chen, Ning Ma, Jen‐taut Yeh

Polymer Engineering & Science · 2024-01 · 64 (1) · 231-242

DOI: 10.1002/pen.26542 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Polymer Engineering & Science, online erschienen am 03.11.2023. Verfasst von Hong‐juan Xu und 4 weiteren Autor:innen. Die Arbeit wurde bisher 5-mal zitiert (Crossref) und nennt 47 Literaturangaben.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Fully renewable oxygen barrier thermoplastic starch (TPS)/sugar alcohol blown films were innovatively prepared by blending proper loadings of Erythritol (ET), Sorbitol (ST), and Lactitol (LT) and supercritical carbon dioxide (scCO 2 ) assistance. The oxygen transmission rate (OTR) values of the properly prepared scCO 2 TPS x ET y , scCO 2 TPS x ST y, and scCO 2 TPS x LT y films reduced to 4.3, 6.6, and 12.5 cm 3 /m 2 ∙day∙atm, which are about 5–28 times smaller than those of the conventional TPS films reported in the literature. The free‐volume‐cavity characteristics (FVCC) and OTR detected for TPS x ET y (or scCO 2 TPS x ET y ), TPS x ST y (or scCO 2 TPS x ST y ), and TPS x LT y (or scCO 2 TPS x LT y ) films diminished to a minimum, as their ET, ST and LT loadings came near an optimal value. Slightly smaller OTR and FVCC values were detected for scCO 2 TPS x ET y , scCO 2 TPS x ST y, and scCO 2 TPS x LT y films than those of corresponding TPS x ET y , TPS x ST y , and TPS x LT y films prepared without scCO 2 ‐assistance. The smallest OTR and FVCC detected for the properly prepared TPS x ET y (or scCO 2 TPS x ET y ), TPS x ST y (or scCO 2 TPS x ST y ), and TPS x LT y (or scCO 2 TPS x LT y ) films diminished with decreasing sugar alcohol's molecular weight. An essential result is that the OTR of the properly prepared scCO 2 TPS x ET y film was merely 4.3 cm 3 /m 2 ∙day∙atm, which is small enough to meet the demand of high oxygen barrier packaging application. Dynamic molecular relaxations detected for these films disclosed that ET, ST, and LT were compatible with TPS, as their loads were ≤ the optimum value. The distinctly reduced OTR and FVCC for these properly prepared films are partially attributed to the reinforced molecular interactions between sugar alcohol and TPS's hydroxyl groups when they were prepared with scCO 2 ‐assistance, optimal sugar alcohol loading, and/or smaller sugar alcohol's molecular weight. Highlights High oxygen barrier thermoplastic starch/sugar alcohol blown films were prepared. The lowest oxygen transmission rate of the renewable film was 4.3 cm 3 /m 2 ∙day∙atm. This oxygen transmission rate is qualified for high oxygen barrier application. Boosted oxygen barrier property was ascribed to the reduced free volume values.

Zitieren

APA

Xu, H., Mei, H., Chen, W., Ma, N., & Yeh, J. (2024). Renewable thermoplastic starch/sugar alcohol blends and their oxygen barrier application. Polymer Engineering & Science, 64(1), 231-242. https://doi.org/10.1002/pen.26542

Vancouver

Xu H, Mei H, Chen W, Ma N, Yeh J. Renewable thermoplastic starch/sugar alcohol blends and their oxygen barrier application. Polymer Engineering & Science. 2024;64(1):231-242. doi:10.1002/pen.26542

BibTeX
@article{Xu2024,
  author = {Xu, Hong‐juan and Mei, Han‐fang and Chen, Wei‐xing and Ma, Ning and Yeh, Jen‐taut},
  title = {Renewable thermoplastic starch/sugar alcohol blends and their oxygen barrier application},
  journal = {Polymer Engineering & Science},
  year = {2024},
  volume = {64},
  number = {1},
  pages = {231--242},
  doi = {10.1002/pen.26542}
}