Sustainable Composites From Almond Shell Powder and Recycled Polyolefin Blends: Effect of Compatibilizer on Interfacial Adhesion and Properties
Polymer Composites · 20.08.2026 · 47 (16) · 14510-14527
DOI: 10.1002/pc.71228 ↗Kurz gefasst
Fachartikel in der Zeitschrift Polymer Composites, online erschienen am 01.06.2026. Verfasst von Rebecca Sanchez und 4 weiteren Autor:innen. Die Arbeit wurde bisher 3-mal zitiert (Crossref) und nennt 62 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY-NC 4.0). Gefördert von: Biomolecular Interaction Centre, University of Canterbury, Ministry of Agriculture, Food and Agribusiness, Natural Sciences and Engineering Research Council of Canada.
Abstract (Originalsprache)
This study reports injection‐molded sustainable composites developed from a hybrid recycled polymer matrix reinforced with agricultural food waste as a biofiller. A 50:50 (w/w) blend of automotive recycled polypropylene and recycled polyolefins derived from industrial pipe‐scrap waste was combined with almond shell powder (ASP) and processed via melt extrusion at 190°C followed by injection molding. Maleic anhydride‐grafted polypropylene was incorporated to enhance polymer–filler interfacial adhesion. Increasing ASP content up to 30 wt.% significantly improved tensile and flexural moduli, heat deflection temperature (HDT), and decreased the linear thermal expansion coefficient (CLTE), reflecting the inherent stiffness of ASP. Rheological analysis showed increased complex viscosity at low frequencies, indicating enhanced polymer–filler interactions. Compatibilization further enhanced tensile strength (~16%), flexural strength (~24%), flexural modulus (~10%), and HDT (~10%), while reducing CLTE (~7.4%) relative to uncompatibilized systems. The composites retained high notched Izod impact strength (> 50 J m −1 ), indicating a favorable balance between stiffness and toughness. Scanning electron microscopy confirmed improved filler dispersion and interfacial bonding. A quantitative correlation between void fraction and stiffness efficiency factor was established, yielding a maximum efficiency of 3.87 with a minimum void content of 0.06%. The sustainable composites maintained low density (< 1 g cm −3 ) and high notched Izod impact strength (> 50 J m −1 ), indicating their suitability for lightweight automotive interior applications.
Förderung
- Biomolecular Interaction Centre, University of Canterbury
- Ministry of Agriculture, Food and Agribusiness
- Natural Sciences and Engineering Research Council of Canada
Zitieren
APA
Sanchez, R., Ghosh, S. K., Alias, N. F., Mohanty, A. K., & Misra, M. (2026). Sustainable Composites From Almond Shell Powder and Recycled Polyolefin Blends: Effect of Compatibilizer on Interfacial Adhesion and Properties. Polymer Composites, 47(16), 14510-14527. https://doi.org/10.1002/pc.71228
Vancouver
Sanchez R, Ghosh SK, Alias NF, Mohanty AK, Misra M. Sustainable Composites From Almond Shell Powder and Recycled Polyolefin Blends: Effect of Compatibilizer on Interfacial Adhesion and Properties. Polymer Composites. 2026;47(16):14510-14527. doi:10.1002/pc.71228
BibTeX
@article{Sanchez2026,
author = {Sanchez, Rebecca and Ghosh, Suman Kumar and Alias, Nur Fazreen and Mohanty, Amar K. and Misra, Manjusri},
title = {Sustainable Composites From Almond Shell Powder and Recycled Polyolefin Blends: Effect of Compatibilizer on Interfacial Adhesion and Properties},
journal = {Polymer Composites},
year = {2026},
volume = {47},
number = {16},
pages = {14510--14527},
doi = {10.1002/pc.71228}
}
EUVIMED