Top‐ and bottom‐of‐the‐line corrosion: Effects of 30 °C bottom liquid and 20 °C steel temperature in CO 2 and H 2 S/N 2 environments
Materialwissenschaft und Werkstofftechnik · 20.11.2026
DOI: 10.1002/mawe.70194 ↗Kurz gefasst
Fachartikel in der Zeitschrift Materialwissenschaft und Werkstofftechnik, online erschienen am 20.11.2026. Verfasst von M. Taqiuddin und 3 weiteren Autor:innen. Die Arbeit nennt 24 Literaturangaben.
Abstract (Originalsprache)
Corrosion in oil and gas pipelines is strongly influenced by environmental chemistry and pipeline location, affecting reliability and safety. This study examines the corrosion behavior of API 5L X65 carbon steel under top (TLC) and bottom (BLC) conditions in sweet (CO 2 ) and sour (H 2 S/N 2 ) environments at 20 °C – 30 °C. Uniform corrosion rates (UCR) and pitting corrosion rates (PCR) were measured using weight loss (ASTM G1‐03) and surface profilometry (ASTM G46‐21), while scanning electron microscopy (SEM), energy dispersive x‐ray spectroscopy (EDX) and x‐ray diffraction (XRD) characterized surface morphology and corrosion products. In the sweet environment, top‐of‐the‐line corrosion and bottom‐of‐the‐line corrosion showed similar uniform corrosion rates (0.28 mm/y). Pitting corrosion was moderate, with pitting corrosion rates of 0.89 mm/y for top‐of‐the‐line corrosion and 0.67 mm/y for bottom‐of‐the‐line corrosion. Products were mainly thin Fe 3 C layers, with NaCl deposition only at the bottom. Under sour conditions, bottom‐of‐the‐line corrosion exhibited higher uniform corrosion rates (0.29 mm/y) than top‐of‐the‐line corrosion (0.22 mm/y), with more severe localized corrosion; pitting corrosion rate reached 1.94 mm/y at bottom‐of‐the‐line corrosion versus 0.43 mm/y at top‐of‐the‐line corrosion. Multilayered FeS scales formed in H 2 S environments, partially protecting the top, while bottom surfaces experienced combined sulfide and chloride attack, promoting localized pitting. These findings show that pipeline corrosion depends strongly on chemical environment and steel position, emphasizing the need for localized monitoring and targeted mitigation strategies to maintain pipeline integrity.
Zitieren
APA
Taqiuddin, M., Othman, N. K., Noor, A. M., & Yaakob, N. (2026). Top‐ and bottom‐of‐the‐line corrosion: Effects of 30 °C bottom liquid and 20 °C steel temperature in CO 2 and H 2 S/N 2 environments. Materialwissenschaft und Werkstofftechnik. https://doi.org/10.1002/mawe.70194
Vancouver
Taqiuddin M, Othman NK, Noor AM, Yaakob N. Top‐ and bottom‐of‐the‐line corrosion: Effects of 30 °C bottom liquid and 20 °C steel temperature in CO 2 and H 2 S/N 2 environments. Materialwissenschaft und Werkstofftechnik. 2026. doi:10.1002/mawe.70194
BibTeX
@article{Taqiuddin2026,
author = {Taqiuddin, M. and Othman, N. Kamil and Noor, A. Md and Yaakob, N.},
title = {Top‐ and bottom‐of‐the‐line corrosion: Effects of 30 °C bottom liquid and 20 °C steel temperature in CO 2 and H 2 S/N 2 environments},
journal = {Materialwissenschaft und Werkstofftechnik},
year = {2026},
doi = {10.1002/mawe.70194}
}