EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Chemically‐Modified Recycled PET/PBT Blends and Their Radio Frequency Welded Bead Foam Structures

Yavuz Akdevelioğlu, Andreas Himmelsbach, Hayden McGreal, Aylin Altınbay, Ehsan Behzadfar, Holger Ruckdäschel, Mohammadreza Nofar

Macromolecular Materials and Engineering · 2026-07 · 311 (7)

DOI: 10.1002/mame.70277 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Macromolecular Materials and Engineering, online erschienen am 13.07.2026. Verfasst von Yavuz Akdevelioğlu und 6 weiteren Autor:innen. Die Arbeit nennt 57 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Türkiye Bilimsel ve Teknolojik Araştirma Kurumu, Deutsche Forschungsgemeinschaft.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

This study investigates the rheological, thermal, bead foaming, and welded bead foam behaviors of recycled polyethylene terephthalate (rPET)/polybutylene terephthalate (PBT) blends modified with a multifunctional epoxy‐based Joncryl chain extender. Three blend weight ratios (75/25, 50/50, and 25/75) were evaluated with and without 1.0 wt.% Joncryl. Bead foams were produced using CO 2 physical blowing agent through continuous extrusion bead foaming. Melt rheological analysis revealed that PBT addition and Joncryl modification increase the complex viscosity and storage modulus of the blends. Differential scanning calorimetry (DSC) and hyper‐DSC analyses confirmed that while co‐crystallization occurs at slow cooling rates, fast cooling of 300°C/min induces crystalline phase immiscibility. This results in clear double‐crystal melting peak formation in all blends and particularly in 50/50 blends. During the radio‐frequency welding, the low‐ and high‐melting‐peak crystals facilitate strong bead‐to‐bead welding and maintain the overall foam structure, respectively. Flexural, tensile, and compressive mechanical analyses demonstrated the presence of stronger inter‐bead welding of the modified 50/50 blends. At this blend ratio, specifically toughness, tensile strength, and strain at break were notably enhanced. Fracture surface analysis of welded bead foams confirmed intra‐bead fracture resulting from high inter‐bead weld strength in all blends.

Förderung

  • Türkiye Bilimsel ve Teknolojik Araştirma Kurumu
  • Deutsche Forschungsgemeinschaft

Zitieren

APA

Akdevelioğlu, Y., Himmelsbach, A., McGreal, H., Altınbay, A., Behzadfar, E., Ruckdäschel, H., & Nofar, M. (2026). Chemically‐Modified Recycled PET/PBT Blends and Their Radio Frequency Welded Bead Foam Structures. Macromolecular Materials and Engineering, 311(7). https://doi.org/10.1002/mame.70277

Vancouver

Akdevelioğlu Y, Himmelsbach A, McGreal H, Altınbay A, Behzadfar E, Ruckdäschel H, et al. Chemically‐Modified Recycled PET/PBT Blends and Their Radio Frequency Welded Bead Foam Structures. Macromolecular Materials and Engineering. 2026;311(7). doi:10.1002/mame.70277

BibTeX
@article{Akdeveliolu2026,
  author = {Akdevelioğlu, Yavuz and Himmelsbach, Andreas and McGreal, Hayden and Altınbay, Aylin and Behzadfar, Ehsan and Ruckdäschel, Holger and Nofar, Mohammadreza},
  title = {Chemically‐Modified Recycled PET/PBT Blends and Their Radio Frequency Welded Bead Foam Structures},
  journal = {Macromolecular Materials and Engineering},
  year = {2026},
  volume = {311},
  number = {7},
  doi = {10.1002/mame.70277}
}
Kostenlos starten →