Kurz gefasst

Fachartikel in der Zeitschrift Global Challenges, online erschienen am 13.11.2026. Verfasst von Asad Ali und 4 weiteren Autor:innen. Beteiligte Einrichtung: School of Engineering Edith Cowan University Joondalup Western Australia Australia. Die Arbeit nennt 59 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Lithium iron phosphate (LFP) batteries dominate electric‐vehicle and stationary‐storage markets, yet their low intrinsic metal value makes lithium recovery from spent material economically challenging. A low‐temperature oxalic acid leaching process recovers lithium from industrial LFP black mass without external oxidants. Box–Behnken response surface methodology (RSM) is combined with kinetic modeling to optimize the process. Temperature (35°C–70°C), oxalic acid concentration (0.30–1.00 M), and solid‐to‐liquid (S/L) ratio (20–100 g L −1 ) are evaluated over 180 min. The S/L ratio dominates lithium extraction, whereas temperature and acid concentration exert weak effects; extraction is essentially complete within 60–90 min. Kinetic analysis indicates that the Avrami model best describes the leaching behavior, consistent with mixed diffusion‐ and reaction‐controlled dissolution. Lithium is released by proton‐driven lattice dissolution while iron precipitates as amorphous iron oxalate, forming a product layer that restricts mass transfer; the low apparent activation energy supports diffusion‐influenced control. Leaching is selective for lithium over iron and copper, but aluminum and phosphorus are co‐extracted and require downstream separation. Under optimized conditions (35°C, 0.71 M oxalic acid, 45.4 g L −1 ), lithium recovery reaches 96%, matching model predictions. Efficient recovery is achievable at low temperature without oxidizing agents, providing a practical basis for sustainable battery recycling.

Schlagwörter

Stichwörter der Autor:innen

battery recyclinghydrometallurgyleachinglithium iron phosphatemixed control mechanismoxalic acidrecycling

Autor:innen und Institutionen

  • School of Engineering Edith Cowan University Joondalup Western Australia Australia.
  • Department of Chemical Engineering University of Gujrat Gujrat Punjab Pakistan.
  • Fraunhofer-Institut für Keramische Technologien und Systeme IKTS Freiberg Germany.
  • Mineral Resource Recovery Centre Edith Cowan University Joondalup Western Australia Australia.

ORCID-Profile: Asad Ali, Amir Razmjou, Muhammad Rizwan Azhar

Zitieren

APA

Ali, A., Arafat, Y., Pavón, S., Razmjou, A., & Azhar, M. R. (2026). Resource Recovery From Spent Lithium Iron Phosphate Batteries via Low‐Temperature Lithium Extraction. Global Challenges, 10(11). https://doi.org/10.1002/gch2.70173

Vancouver

Ali A, Arafat Y, Pavón S, Razmjou A, Azhar MR. Resource Recovery From Spent Lithium Iron Phosphate Batteries via Low‐Temperature Lithium Extraction. Global Challenges. 2026;10(11). doi:10.1002/gch2.70173

BibTeX
@article{Ali2026,
  author = {Ali, Asad and Arafat, Yasir and Pavón, Sandra and Razmjou, Amir and Azhar, Muhammad Rizwan},
  title = {Resource Recovery From Spent Lithium Iron Phosphate Batteries via Low‐Temperature Lithium Extraction},
  journal = {Global Challenges},
  year = {2026},
  volume = {10},
  number = {11},
  doi = {10.1002/gch2.70173}
}
Kostenlos starten →