EUVIMEDEUVIMED entdecken
Open Access · CC BY-NC-ND 4.0

Mechanochemical Degradation and Fluoride Recovery of Perfluorosulfonic Acid Polymer Membrane

Valentin Monjal, Guillaume Cazals, Xavier Bantreil, Frédéric Lamaty, Bruno Ameduri iD

ChemSusChem · 14.08.2026 · 19 (15)

DOI: 10.1002/cssc.70924 ↗

Kurz gefasst

Fachartikel in der Zeitschrift ChemSusChem, online erschienen am 03.08.2026. Verfasst von Valentin Monjal und 4 weiteren Autor:innen. Beteiligte Einrichtung: Institute Charles Gerhardt, CNRS, ENSCM, Université de Montpellier, Montpellier, France. Die Arbeit wurde bisher 1-mal zitiert (Crossref) und nennt 67 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY-NC-ND 4.0). Gefördert von: PEPR.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Per‐ or polyfluoroalkyl substances (PFAS) represent a large family of chemicals, widely used due to their outstanding properties. However, also known as “Forever Chemicals”, they are raising attention due to high health and environmental risks. In last years, the elimination, degradation, or recycling of PFAS has become essential. In this work, the degradation of a perfluorosulfonic acid polymer, Nafion, composed of a poly(tetrafluoroethylene) backbone with perfluoroether side chains terminated by sulfonic acid groups, is studied. More precisely, the mechanochemical degradation, previously described for linear fluoropolymers, is reported on branched PFSA polymers in the presence of various activators (such as (pyro)phosphates, 1,8‐Diazabicyclo [5.4.0]undec‐7‐ene (DBU), 1,5,7‐Triazabicyclo [4.4.0]dec‐5‐ene(TBD), KOH) at room temperature. Recovered products were characterized over time by nuclear magnetic resonance and Fourier transformation infrared spectroscopy, scanning electron microscopy–energy dispersive X‐ray spectroscopy, and liquid chromatography–mass spectrometry in order to both identify the released products and suggest a degradation pathway. The use of potassium hydroxide, although resulting in a moderate potassium fluoride yield, allowed the determination of fragments produced during the degradation mechanism, while others were ineffective. Phosphate salts have been revealed to be the best candidates enabling the mineralization of PFSA, yielding valuable products and a good fluorine recovery for a further circular economy.

Schlagwörter

Stichwörter der Autor:innen

degradationfluoropolymersmechanochemistryperfluorosulfonic acidrecycling

Autor:innen und Institutionen

  • Institute Charles Gerhardt, CNRS, ENSCM, Université de Montpellier, Montpellier, France.
  • PAC Chimie Balard, CNRS, ENSCM, Université de Montpellier, Montpellier, France.
  • Institut Des Biomolécules Max Mousseron, CNRS, ENSCM, Université de Montpellier, Montpellier, France.
  • Institut Universitaire de France (IUF), Paris, France.

ORCID-Profile: Bruno Ameduri

Förderung

  • PEPR

Zitieren

APA

Monjal, V., Cazals, G., Bantreil, X., Lamaty, F., & Ameduri, B. (2026). Mechanochemical Degradation and Fluoride Recovery of Perfluorosulfonic Acid Polymer Membrane. ChemSusChem, 19(15). https://doi.org/10.1002/cssc.70924

Vancouver

Monjal V, Cazals G, Bantreil X, Lamaty F, Ameduri B. Mechanochemical Degradation and Fluoride Recovery of Perfluorosulfonic Acid Polymer Membrane. ChemSusChem. 2026;19(15). doi:10.1002/cssc.70924

BibTeX
@article{Monjal2026,
  author = {Monjal, Valentin and Cazals, Guillaume and Bantreil, Xavier and Lamaty, Frédéric and Ameduri, Bruno},
  title = {Mechanochemical Degradation and Fluoride Recovery of Perfluorosulfonic Acid Polymer Membrane},
  journal = {ChemSusChem},
  year = {2026},
  volume = {19},
  number = {15},
  doi = {10.1002/cssc.70924}
}
Kostenlos starten →