The Influence of Deep Margin Elevation and Immediate Dentin Sealing on the Fracture Strength of Premolars Restored With Indirect Inlays: An In Vitro Study

Lulwa E Al-Turki iD, Osamah A Alsulimani iD, Khadijah M Baik iD, Haytham Othmani, Naif M Alqarni, Abdullah A Alqarni, Raghad A Al-Dabbagh iD

Clinical and Experimental Dental Research · 2025-06 · 11 (3)

DOI: 10.1002/cre2.70161 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Clinical and Experimental Dental Research, online erschienen am 24.06.2025. Verfasst von Lulwa E Al-Turki und 6 weiteren Autor:innen. Beteiligte Einrichtung: Department of Oral Maxillofacial Prosthodontics, Faculty of Dentistry, King Abdulaziz University, Jeddah, Makkah Province, Saudi Arabia. Hauptthemen laut MEDLINE: Bicuspid, Inlays, Tooth Fractures, Dentin. Die Arbeit wurde bisher 3-mal zitiert (Crossref) und nennt 28 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: This study was funded from King Abdulaziz University, General Program (G: 508-165-1439)..

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Objective

To evaluate the effect of deep margin elevation (DME) and immediate dentin sealing (IDS) on the fracture strength of premolars restored with lithium disilicate inlay restorations. Materials and Methods Standard MOD inlays with proximal box preparations extending 3 mm apical to the cementoenamel junction were prepared on forty sound premolars ( n = 10) randomly divided into four groups: inlays without DME and without IDS (G1); inlays without DME but with IDS (G2); inlays with DME but without IDS (G3); and inlays with both techniques applied (G4). Composite resin was applied incrementally to elevate the proximal cervical margin coronally to the cementoenamel junction. For immediate dentin sealing, bonding agent was applied immediately after tooth preparation. All teeth were restored with lithium disilicate inlays and, after adhesive resin cementation, specimens were thermomechanically aged for 500 cycles at 5°–55°C and then subjected to load failure testing. Failure loads and locations were recorded and analyzed using one‐ and two‐way ANOVA with Tukey's post‐hoc testing ( α = 0.05). Failure modes were analyzed using descriptive statistics.

Results

The mean fracture loads were 565.76 ± 233.22 N, 978.47 ± 394.2 N, 974.31 ± 334.7 N, and 1108.21 ± 292.41 N for G1, G2, G3, and G4, respectively. Deep margin elevation ( p = 0.011) and immediate dentin sealing ( p = 0.010) were associated with significantly increased fracture loads. Fracture loads were significantly lower for G1 teeth than for G2‐G4 teeth, but there were no significant differences between G2, G3, and G4. G1 teeth showed 50% catastrophic and non‐catastrophic failures, which increased to 60% for G2 and decreased to 20% for G3 teeth. Samples with both seals and elevation (G4) had a 60% catastrophic failure rate.

Conclusions

When applied individually or together, deep margin elevation and immediate dentin sealing significantly increase the fracture strength of premolars restored with indirect lithium disilicate inlays. Clinical Implications In the challenging setting of margin elevation, studies on the effects of immediate dentin sealing have generally been limited to evaluating marginal integrity and bond strength. The findings of this In Vitro study suggest that both deep margin elevation and immediate dentin sealing protocols are likely to improve clinical outcomes of indirect lithium disilicate inlay restorations and may be considered viable options in clinical practice.

Schlagwörter

MeSH-Schlagwörter (MEDLINE)

BicuspidInlaysTooth FracturesDentinHumansIn Vitro TechniquesComposite ResinsDentin-Bonding AgentsDental PorcelainDental Stress AnalysisDental Restoration FailureDental Bonding

Stichwörter der Autor:innen

deep margin elevationdentin sealingfracture strengthlithium disilicate inlay restorations

Substanzen

Composite Resinslithia disilicateDentin-Bonding AgentsDental Porcelain

Autor:innen und Institutionen

  • Department of Oral Maxillofacial Prosthodontics, Faculty of Dentistry, King Abdulaziz University, Jeddah, Makkah Province, Saudi Arabia.
  • Department of Oral Diagnostic Sciences, Faculty of Dentistry, King Abdulaziz University, Jeddah, Makkah Province, Saudi Arabia.
  • Choueifat Medical Center, Jeddah, Makkah Province, Saudi Arabia.
  • Al-Rahaily medical Center, Jeddah, Makkah Province, Saudi Arabia.
  • Periodontics Resident, King Fahad General hospital, Jeddah, Makkah Province, Saudi Arabia.

ORCID-Profile: Lulwa E Al-Turki, Osamah A Alsulimani, Khadijah M Baik, Raghad A Al-Dabbagh

Förderung

  • This study was funded from King Abdulaziz University, General Program (G: 508-165-1439).

Zitieren

APA

Al-Turki, L. E., Alsulimani, O. A., Baik, K. M., Othmani, H., Alqarni, N. M., Alqarni, A. A., & Al-Dabbagh, R. A. (2025). The Influence of Deep Margin Elevation and Immediate Dentin Sealing on the Fracture Strength of Premolars Restored With Indirect Inlays: An In Vitro Study. Clinical and Experimental Dental Research, 11(3). https://doi.org/10.1002/cre2.70161

Vancouver

Al-Turki LE, Alsulimani OA, Baik KM, Othmani H, Alqarni NM, Alqarni AA, et al. The Influence of Deep Margin Elevation and Immediate Dentin Sealing on the Fracture Strength of Premolars Restored With Indirect Inlays: An In Vitro Study. Clinical and Experimental Dental Research. 2025;11(3). doi:10.1002/cre2.70161

BibTeX
@article{AlTurki2025,
  author = {Al-Turki, Lulwa E and Alsulimani, Osamah A and Baik, Khadijah M and Othmani, Haytham and Alqarni, Naif M and Alqarni, Abdullah A and Al-Dabbagh, Raghad A},
  title = {The Influence of Deep Margin Elevation and Immediate Dentin Sealing on the Fracture Strength of Premolars Restored With Indirect Inlays: An In Vitro Study},
  journal = {Clinical and Experimental Dental Research},
  year = {2025},
  volume = {11},
  number = {3},
  doi = {10.1002/cre2.70161}
}
Kostenlos starten →