Quantifying Per‐Pulse Growth of BiOI for Thickness Optimization of Converted BiVO 4 Photoanodes
ChemPhotoChem · 2026-11 · 10 (11)
DOI: 10.1002/cptc.70335 ↗Kurz gefasst
Fachartikel in der Zeitschrift ChemPhotoChem, online erschienen am 30.10.2026. Verfasst von Moeka Hie und 5 weiteren Autor:innen. Die Arbeit nennt 42 Literaturangaben. Gefördert von: Japan Society for the Promotion of Science, Tokyo Ohka Foundation for The Promotion of Science and Technology, New Energy and Industrial Technology Development Organization.
Abstract (Originalsprache)
Precise thickness control is essential for optimizing BiVO 4 photoanodes because increasing film thickness enhances visible‐light absorption but can simultaneously aggravate carrier‐transport loss. Here, we report a pulse‐electrodeposition route for the fabrication of BiVO 4 /FTO photoanodes via BiOI precursor films and compare it with conventional continuous electrodeposition. Pulse electrodeposition enabled cycle‐resolved growth of BiVO 4 with an average thickness increment of 34.0 nm per cycle and allowed film thicknesses up to ~1700 nm without severe delamination from the FTO conductive substrate, whereas continuous electrodeposition reached a thickness limit of ~600 nm. Structural analyses revealed that pulse‐electrodeposition modified the internal growth structure of the precursor and converted films while maintaining the same BiVO 4 phase identity. Photoelectrochemical measurements under simulated AM 1.5G illumination showed that the photocurrent density at 1.23 V RHE increased with pulse cycle number up to 25 cycles and then decreased at higher cycle numbers, reaching a maximum of 3.5 ± 0.1 mA cm −2 , significantly higher than that of an electrodeposition‐time‐matched continuous reference (approximately 1.2 mA cm −2 ). Optical, IPCE, and numerical analyses indicate that this optimum arises from a trade‐off between enhanced light harvesting below a critical thickness of approximately 850 nm and increasing carrier‐transport/recombination losses at larger thicknesses.
Förderung
- Japan Society for the Promotion of Science
- Tokyo Ohka Foundation for The Promotion of Science and Technology
- New Energy and Industrial Technology Development Organization
Zitieren
APA
Hie, M., Nandal, V., Yoshiyama, K., Xiao, T., Seki, K., & Higashi, T. (2026). Quantifying Per‐Pulse Growth of BiOI for Thickness Optimization of Converted BiVO 4 Photoanodes. ChemPhotoChem, 10(11). https://doi.org/10.1002/cptc.70335
Vancouver
Hie M, Nandal V, Yoshiyama K, Xiao T, Seki K, Higashi T. Quantifying Per‐Pulse Growth of BiOI for Thickness Optimization of Converted BiVO 4 Photoanodes. ChemPhotoChem. 2026;10(11). doi:10.1002/cptc.70335
BibTeX
@article{Hie2026,
author = {Hie, Moeka and Nandal, Vikas and Yoshiyama, Koichi and Xiao, Tian and Seki, Kazuhiko and Higashi, Tomohiro},
title = {Quantifying Per‐Pulse Growth of BiOI for Thickness Optimization of Converted BiVO 4 Photoanodes},
journal = {ChemPhotoChem},
year = {2026},
volume = {10},
number = {11},
doi = {10.1002/cptc.70335}
}
EUVIMED