Fachartikel in der Zeitschrift Angewandte Chemie International Edition, online erschienen am 05.11.2026. Verfasst von Zi-Rui Li und 5 weiteren Autor:innen. Beteiligte Einrichtung: Department of Chemistry, Hefei National Research Center for Physical Sciences at the Microscale, University of Science and Technology of China, Hefei…. Die Arbeit nennt 46 Literaturangaben. Gefördert von: National Natural Science Foundation of China, Anhui Provincial Natural Science Foundation, Fundamental Research Funds for the Central Universities.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Improving the durability of platinum (Pt)‐based catalysts for the oxygen reduction reaction (ORR) remains a central challenge in the commercialization of proton exchange membrane fuel cells (PEMFCs), yet simple and effective indicators to guide the rational design of highly stable Pt‐based catalysts are still lacking. Herein, we identify initial electrochemically active surface area (ECSA) and dry proton accessibility (DPA) as two key indicators for unraveling cathodic Pt/C catalyst degradation. Systematic studies on a library of Pt/C catalysts with a wide range of initial ECSA (49–114 m 2 g Pt −1 ) and DPA (27%–91%) reveal clear relationships between these two indicators and ECSA loss: at a comparable DPA, ECSA loss decreases significantly with the reduction in initial ECSA; at a similar initial ECSA, lower DPA effectively mitigates ECSA loss; and the influence of DPA on ECSA loss becomes increasingly prominent as initial ECSA decreases. Regression analysis further clarifies the respective roles of these two indicators: initial ECSA is the dominant factor associated with ECSA loss within the catalyst library, while DPA further modulates degradation depending on the initial ECSA level. These findings suggest that catalyst durability can be improved by prioritizing the reduction of initial ECSA, with further benefits achieved by lowering DPA.

Schlagwörter

Stichwörter der Autor:innen

dry proton accessibilitydurability indicatorselectrochemical surface areaproton exchange membrane fuel cells

Autor:innen und Institutionen

  • Department of Chemistry, Hefei National Research Center for Physical Sciences at the Microscale, University of Science and Technology of China, Hefei, China.

ORCID-Profile: Lei Tong, Ru-Yang Shao, Hai-Wei Liang

Förderung

  • National Natural Science Foundation of China
  • Anhui Provincial Natural Science Foundation
  • Fundamental Research Funds for the Central Universities
  • Natural Science Foundation of Anhui Province

Zitieren

APA

Li, Z. R., Tong, L., Xu, C., Song, T. W., Shao, R. Y., & Liang, H. W. (2026). Electrochemical Indicators for Designing Durable Low‐Pt Fuel Cell Catalysts. Angewandte Chemie International Edition. https://doi.org/10.1002/anie.7149274

Vancouver

Li ZR, Tong L, Xu C, Song TW, Shao RY, Liang HW. Electrochemical Indicators for Designing Durable Low‐Pt Fuel Cell Catalysts. Angewandte Chemie International Edition. 2026. doi:10.1002/anie.7149274

BibTeX
@article{Li2026,
  author = {Li, Zi-Rui and Tong, Lei and Xu, Cong and Song, Tian-Wei and Shao, Ru-Yang and Liang, Hai-Wei},
  title = {Electrochemical Indicators for Designing Durable Low‐Pt Fuel Cell Catalysts},
  journal = {Angewandte Chemie International Edition},
  year = {2026},
  doi = {10.1002/anie.7149274}
}
Kostenlos starten →