EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Stabilizing Configurational Entropy in Spinel‐type High Entropy Oxides during Discharge–Charge by Overcoming Kinetic Sluggish Diffusion

Ke Li, Lingfeng Shi, Jiale An, Mengjie Zhang, Yang Du, Yulin Ma, Shuaifeng Lou, Geping Yin, Zhenjiang Yu iD, Xiao Hua, Hua Huo

Angewandte Chemie International Edition · 15.12.2025 · 64 (51)

DOI: 10.1002/anie.202518569 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Angewandte Chemie International Edition, online erschienen am 06.11.2025. Verfasst von Ke Li und 10 weiteren Autor:innen. Beteiligte Einrichtung: State Key Laboratory of Space Power-Sources, School of Chemistry and Chemical Engineering, Harbin Institute of Technology, Harbin, 150001, China. Die Arbeit wurde bisher 15-mal zitiert (Crossref) und nennt 59 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Natural Science Foundation of China.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Spinel‐type high entropy oxides (HEOs) have emerged as promising next‐generation lithium‐ion battery anodes owing to exceptional electrochemical performance. However, suppressing irreversible phase transformations caused by high‐entropy to low‐entropy state transitions during discharge–charge has remained challenging. The core issue stems from an insufficient understanding of phase evolution pathways and the key thermodynamic/kinetic driving forces, which is due to current methodological limitations in analyzing highly disordered structures. Further complicating this challenge is the elusive impact of nanosized effects on both thermodynamic and kinetic processes. This study addresses these challenges through three synergistic approaches: 1) investigating phase evolution mechanisms across different particle sizes to delineate nanosized effects; 2) resolving complex local structures by pair distribution function analyses and 7 Li magic‐angle spinning nuclear magnetic resonance spectroscopy; 3) elucidating influences of high entropy on phase evolution via DFT calculations. Comprehensive results reveal a complex phase evolution process governed by the thermodynamic‐kinetic interplay. The incomplete phase transformations of the rock‐salt‐like intermediate phase during discharge, which are attributable to high entropy‐mediated kinetic sluggish diffusion, account for the transition from high‐entropy to low‐entropy states. By shortening the solid‐state diffusion lengths, the kinetic limitations can be overcome, as demonstrated by nanosized spinel‐type HEOs achieving reversible phase transformations during discharge‐charge.

Schlagwörter

Stichwörter der Autor:innen

High entropy oxidesKinetic sluggish diffusionLithium‐ion batteriesNanosized effectsPhase evolution pathways

Autor:innen und Institutionen

  • State Key Laboratory of Space Power-Sources, School of Chemistry and Chemical Engineering, Harbin Institute of Technology, Harbin, 150001, China.
  • Department of Chemistry, Lancaster University, Lancaster, LA1 4YB, UK.

ORCID-Profile: Zhenjiang Yu

Förderung

  • National Natural Science Foundation of China

Zitieren

APA

Li, K., Shi, L., An, J., Zhang, M., Du, Y., Ma, Y., Lou, S., Yin, G., Yu, Z., Hua, X., & Huo, H. (2025). Stabilizing Configurational Entropy in Spinel‐type High Entropy Oxides during Discharge–Charge by Overcoming Kinetic Sluggish Diffusion. Angewandte Chemie International Edition, 64(51). https://doi.org/10.1002/anie.202518569

Vancouver

Li K, Shi L, An J, Zhang M, Du Y, Ma Y, et al. Stabilizing Configurational Entropy in Spinel‐type High Entropy Oxides during Discharge–Charge by Overcoming Kinetic Sluggish Diffusion. Angewandte Chemie International Edition. 2025;64(51). doi:10.1002/anie.202518569

BibTeX
@article{Li2025,
  author = {Li, Ke and Shi, Lingfeng and An, Jiale and Zhang, Mengjie and Du, Yang and Ma, Yulin and Lou, Shuaifeng and Yin, Geping and Yu, Zhenjiang and Hua, Xiao and Huo, Hua},
  title = {Stabilizing Configurational Entropy in Spinel‐type High Entropy Oxides during Discharge–Charge by Overcoming Kinetic Sluggish Diffusion},
  journal = {Angewandte Chemie International Edition},
  year = {2025},
  volume = {64},
  number = {51},
  doi = {10.1002/anie.202518569}
}
Kostenlos starten →