Fachartikel in der Zeitschrift Angewandte Chemie International Edition, online erschienen am 26.09.2025. Verfasst von Yuxin Yuan und 6 weiteren Autor:innen. Beteiligte Einrichtung: School of Chemistry and Chemical Engineering, Shanghai Jiao Tong University, Shanghai, 200240, P.R. China. Die Arbeit wurde bisher 25-mal zitiert (Crossref) und nennt 62 Literaturangaben. Gefördert von: National Natural Science Foundation of China.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Aqueous zinc‐ion batteries (AZIBs) are promising high‐safety energy storage devices, but their practical implementation has been limited by dendrite growth and hydrogen evolution reaction (HER). Solid‐electrolyte interface (SEI) is expected to address these problems. Herein, we revealed that HER results in loose and porous interfacial structure, making the in situ construction of reliable SEI a challenge. Thus, a universal and effective hydrogen atom scavenging strategy is proposed to in situ construct a dense and uniform inorganic SEI by introducing potassium persulfate (PSS). PSS scavenges the adsorbed hydrogen atoms, thus inhibiting HER. Meanwhile, PSS is reduced into SO 4 2− and participates in the formation of zinc hydroxide sulfates (ZHS). With no interference of H 2 bubbles on ZHS crystallization, an ideal SEI is constructed. This ZHS‐SEI exhibits superior electronic insulation, effectively suppressing further HER and Zn dendrite growth during cycling. As a result, the Zn//Zn symmetric cell with PSS can achieve stable Zn plating/stripping for 1882 h at 5 mA cm −2 and 2.5 mAh cm −2 and 650 h at 10 mA cm −2 and 5 mAh cm −2 , respectively. The cycling stability of the Zn||NVO full cell is also significantly improved at 5 A g −1 . This work provides a novel perspective for stabilizing the zinc anode interface.

Schlagwörter

Stichwörter der Autor:innen

Aqueous Zn‐ion batteriesHydrogen atom captureHydrogen evolution reactionSolid electrolyte interfaceZn metal anode

Autor:innen und Institutionen

  • School of Chemistry and Chemical Engineering, Shanghai Jiao Tong University, Shanghai, 200240, P.R. China.
  • School of Materials Science and Engineering, Tongji University, Shanghai, 201804, P.R. China.
  • State Key Laboratory of Clean and Efficient Coal Utilization, Taiyuan University of Technology, Taiyuan, 030024, P.R. China.

Förderung

  • National Natural Science Foundation of China

Zitieren

APA

Yuan, Y., Chen, J., Qian, T., Zhang, B., Ye, K., Li, R., & Yang, X. (2025). Hydrogen Atom Capture Toward Dense Solid Electrolyte Interface for Long‐Cycling Aqueous Zinc‐Ion Batteries. Angewandte Chemie International Edition, 64(48). https://doi.org/10.1002/anie.202513722

Vancouver

Yuan Y, Chen J, Qian T, Zhang B, Ye K, Li R, et al. Hydrogen Atom Capture Toward Dense Solid Electrolyte Interface for Long‐Cycling Aqueous Zinc‐Ion Batteries. Angewandte Chemie International Edition. 2025;64(48). doi:10.1002/anie.202513722

BibTeX
@article{Yuan2025,
  author = {Yuan, Yuxin and Chen, Jianping and Qian, Tianyue and Zhang, Bowen and Ye, Ke and Li, Ruimin and Yang, Xiaowei},
  title = {Hydrogen Atom Capture Toward Dense Solid Electrolyte Interface for Long‐Cycling Aqueous Zinc‐Ion Batteries},
  journal = {Angewandte Chemie International Edition},
  year = {2025},
  volume = {64},
  number = {48},
  doi = {10.1002/anie.202513722}
}
Kostenlos starten →