High‐Entropy Aqueous Electrolyte Induced Formation of Water‐Poor Zn 2+ Solvation Structures and Gradient Solid‐Electrolyte Interphase for Long‐Life Zn‐Metal Anodes
Angewandte Chemie International Edition · 07.04.2025 · 64 (15)
DOI: 10.1002/anie.202425008 ↗Kurz gefasst
Fachartikel in der Zeitschrift Angewandte Chemie International Edition, online erschienen am 05.02.2025. Verfasst von Lin Lin und 12 weiteren Autor:innen. Beteiligte Einrichtung: National Laboratory of Solid State Microstructures, College of Engineering and Applied Sciences, Jiangsu Key Laboratory of Artificial Functional Mate…. Die Arbeit wurde bisher 77-mal zitiert (Crossref) und nennt 49 Literaturangaben. Gefördert von: Fundamental Research Funds for the Central Universities, National Natural Science Foundation of China, the National Key R&D Program of China.
Abstract (Originalsprache)
Electrolyte engineering has emerged as an effective strategy for stabilizing Zn‐metal anodes. However, a single solute or solvent additive is far from sufficient to meet the requirements for electrolyte cycling stability. Here, we report a new‐type high‐entropy electrolyte composed of equal molar amounts of Zn(OTf) 2 and LiOTf, along with equal volumes of H 2 O, triethyl phosphate, and dimethyl sulfoxide, which enhances electrolyte stability by increasing solvation entropy. Specifically, this well‐designed high‐entropy electrolyte reduces the content of solvated and free water molecules while forming a robust gradient solid‐electrolyte interphase on the Zn anode surface, protecting the Zn anode from water‐induced corrosion. Moreover, the cationic electrostatic shielding layer on the Zn anode effectively suppresses the “tip effect”, enabling the uniform deposition of Zn. The synergistic effects of this mixed electrolyte effectively leverage the properties of individual additives, significantly extending the cycle life of Zn‐metal anodes. Consequently, the resulting Zn//Zn symmetric cell using this high‐entropy electrolyte can operate over 8000 h at 1 mA cm −2 and 0.5 mAh cm −2 . To highlight, in a Zn//V 2 O 5 ⋅H 2 O pouch cell, it retains 83.1 % of initial capacity after 420 cycles at 1 A g −1 . Such multifunctional high‐entropy electrolyte design provides a meaningful reference for stable Zn‐metal anodes.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- National Laboratory of Solid State Microstructures, College of Engineering and Applied Sciences, Jiangsu Key Laboratory of Artificial Functional Materials, Collaborative Innovation Center of Advanced Microstructures, Na…
- Henan Key Laboratory of New Optoelectronic Functional Materials, College of Chemistry and Chemical Engineering, Anyang Normal University, Anyang, 455000, P. R. China.
- Department of Materials Science and Engineering & Center of Super-Diamond and Advanced Films, City University of Hong Kong, Hong Kong SAR, 999077, P. R. China.
- Institute of Emergency Science, Chinese Institute of Coal Science, Beijing, 100013, P. R. China.
- Key Laboratory of Multifunctional Nanomaterials and Smart Systems, Suzhou Institute of Nano-Tech and Nano-Bionics, Chinese Academy of Sciences, Suzhou, 215123, P. R. China.
ORCID-Profile: Yagang Yao
Förderung
- Fundamental Research Funds for the Central Universities
- National Natural Science Foundation of China
- the National Key R&D Program of China
- the Suzhou Institute of Nano-Tech and Nano-Bionics, Chinese Academy of Sciences
- the Project of Science and Technology Innovation and Entrepreneurship Fund of China Coal Technology & Engineering Group Co., Ltd.
Zitieren
APA
Lin, L., Shao, Z., Liu, S., Yang, P., Zhu, K., Zhuang, W., Li, C., Guo, G., Wang, W., Hong, G., Wu, B., Zhang, Q., & Yao, Y. (2025). High‐Entropy Aqueous Electrolyte Induced Formation of Water‐Poor Zn 2+ Solvation Structures and Gradient Solid‐Electrolyte Interphase for Long‐Life Zn‐Metal Anodes. Angewandte Chemie International Edition, 64(15). https://doi.org/10.1002/anie.202425008
Vancouver
Lin L, Shao Z, Liu S, Yang P, Zhu K, Zhuang W, et al. High‐Entropy Aqueous Electrolyte Induced Formation of Water‐Poor Zn 2+ Solvation Structures and Gradient Solid‐Electrolyte Interphase for Long‐Life Zn‐Metal Anodes. Angewandte Chemie International Edition. 2025;64(15). doi:10.1002/anie.202425008
BibTeX
@article{Lin2025,
author = {Lin, Lin and Shao, Zhipeng and Liu, Shizhuo and Yang, Peng and Zhu, Kaiping and Zhuang, Wubin and Li, Chaowei and Guo, Gengde and Wang, Wenhui and Hong, Guo and Wu, Bing and Zhang, Qichong and Yao, Yagang},
title = {High‐Entropy Aqueous Electrolyte Induced Formation of Water‐Poor Zn 2+ Solvation Structures and Gradient Solid‐Electrolyte Interphase for Long‐Life Zn‐Metal Anodes},
journal = {Angewandte Chemie International Edition},
year = {2025},
volume = {64},
number = {15},
doi = {10.1002/anie.202425008}
}
EUVIMED