Stabilizing Interfaces in High‐Temperature NCM811‐Li Batteries via Tuning Terminal Alkyl Chains of Ether Solvents

Zhijie Wang, Changsheng Chen, Danni Wang, Ye Zhu, Biao Zhang

Angewandte Chemie International Edition · 10.07.2023 · 62 (28)

DOI: 10.1002/anie.202303950 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Angewandte Chemie International Edition, online erschienen am 31.05.2023. Verfasst von Zhijie Wang und 4 weiteren Autor:innen. Beteiligte Einrichtung: Department of Applied Physics & Research Institute for Smart Energy, The Hong Kong Polytechnic University, Hung Hom, Hong Kong, 999077, P. R. China. Die Arbeit wurde bisher 108-mal zitiert (Crossref) und nennt 65 Literaturangaben. Gefördert von: Hong Kong Research Grants Council, Hong Kong Polytechnic University.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Ether electrolytes are promising for lithium metal batteries. Despite the intensive research in recent years, most state‐of‐the‐art ether electrolytes still cannot form reliable electrode‐electrolyte interfaces in NCM811‐Li batteries at diluted concentrations, especially in those operating at elevated temperatures. We report a simple but effective strategy to break this bottleneck and stabilize interfaces in high‐temperature NCM811‐Li batteries in ether electrolytes. We propose that by gradually extending the terminal groups of glycol diethers from methyl groups to n ‐butyl groups, the comprehensive stability of ether electrolytes is improved. An anion‐dominated solvation structure is realized at a concentration of 1 M. Accordingly, the electrode‐electrolyte interactions are suppressed, and a thinner, denser, and more inorganic‐rich solid‐ /cathode‐electrolyte interface is achieved. Additionally, the surface phase transition and structural degradation of NCM811 cathode are alleviated. Consequently, in the ethylene glycol dibutyl ether‐based electrolyte, the Coulombic efficiency for Li−Cu cells working at 60 °C is boosted to 99.41 % with a cycling life of over 200 cycles. The lifespan of high‐temperature NCM811‐Li cells is prolonged by more than 400 % with a stable average Coulombic efficiency of 99.77 % at quasi‐practical conditions of 50 μm Li, lean electrolyte of 10 μL mAh −1 , and medium‐high cathode loading of >2.2 mAh cm −2 .

Schlagwörter

Stichwörter der Autor:innen

Alkoxy GroupsElectrode-Electrolyte InterfacesEther ElectrolytesHigh-Temperature NCM811-Li BatteriesTerminal Alkyl Chains

Autor:innen und Institutionen

  • Department of Applied Physics & Research Institute for Smart Energy, The Hong Kong Polytechnic University, Hung Hom, Hong Kong, 999077, P. R. China.

Förderung

  • Hong Kong Research Grants Council
  • Hong Kong Polytechnic University

Zitieren

APA

Wang, Z., Chen, C., Wang, D., Zhu, Y., & Zhang, B. (2023). Stabilizing Interfaces in High‐Temperature NCM811‐Li Batteries via Tuning Terminal Alkyl Chains of Ether Solvents. Angewandte Chemie International Edition, 62(28). https://doi.org/10.1002/anie.202303950

Vancouver

Wang Z, Chen C, Wang D, Zhu Y, Zhang B. Stabilizing Interfaces in High‐Temperature NCM811‐Li Batteries via Tuning Terminal Alkyl Chains of Ether Solvents. Angewandte Chemie International Edition. 2023;62(28). doi:10.1002/anie.202303950

BibTeX
@article{Wang2023,
  author = {Wang, Zhijie and Chen, Changsheng and Wang, Danni and Zhu, Ye and Zhang, Biao},
  title = {Stabilizing Interfaces in High‐Temperature NCM811‐Li Batteries via Tuning Terminal Alkyl Chains of Ether Solvents},
  journal = {Angewandte Chemie International Edition},
  year = {2023},
  volume = {62},
  number = {28},
  doi = {10.1002/anie.202303950}
}
Kostenlos starten →