Temperature‐Inert Interface Enables Safe and Practical Energy‐Dense LiNi 0.91 Co 0.07 Mn 0.02 O 2 Pouch Cells

Junxian Hou, Qinyu Shi, Xuning Feng, Junpei Terada, Li Wang, Liqi Zhao, Daihua Cao, Shigeaki Yamazaki, Chengshan Xu, Yue Qiu, Jing Feng, Toshiharu Shimooka und 6 weitere

Advanced Energy Materials · 2024-10 · 14 (40)

DOI: 10.1002/aenm.202402638 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Advanced Energy Materials, online erschienen am 20.07.2024. Verfasst von Junxian Hou und 17 weiteren Autor:innen. Die Arbeit wurde bisher 28-mal zitiert (Crossref) und nennt 57 Literaturangaben. Gefördert von: National Natural Science Foundation of China, Fundamental Research Funds for the Central Universities.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Safety concerns significantly hinder the practical implementation of ultrahigh‐nickel cathodes in lithium‐ion batteries. The solid electrolyte interphase (SEI) derived from conventional ester‐based electrolyte is susceptible to thermal decomposition, resulting in battery safety degradation. Herein, a temperature‐inert and inorganic‐rich SEI is developed for the ultrahigh‐nickel LiNi 0.91 Co 0.07 Mn 0.02 O 2 |graphite (NCM91|Gr) battery by employing a flame‐retardant diluted weakly solvated electrolyte. Temperature‐dependent X‐ray photoelectron spectroscopy reveals that SEI's inorganic components of LiF, Li 2 SO 3 , Li 2 SO 4 , and Li 3 N exhibit exceptional thermotolerance under thermal attack. Further evidence from temperature‐dependent X‐ray diffraction indicates that this thermally stable interface effectively mitigates the anode phase transition from the original LiC 6 to LiC 12 state, resulting in a remarkable improvement in intrinsic safety and a 32% reduction in gas emission for battery. The 1.2 Ah NCM91|Gr pouch cell exhibits a thermal failure onset temperature as high as 183.1 °C and maintains stability at 180 °C for 60 min. Furthermore, a 360 Wh kg −1 12.3 Ah LiNi 0.92 Co 0.06 Mn 0.02 O 2 |graphite@20% silicon dioxide cell experiences no thermal runaway even at 200 °C. The 1.2 Ah NCM91|Gr pouch cell also delivers outstanding capacity retention of 90.5% after 1200 cycles with enhanced electrochemical performance. This study provides a promising approach for developing safer energy‐dense batteries through electrolyte and interface design.

Förderung

  • National Natural Science Foundation of China
  • Fundamental Research Funds for the Central Universities

Zitieren

APA

Hou, J., Shi, Q., Feng, X., Terada, J., Wang, L., Zhao, L., Cao, D., Yamazaki, S., Xu, C., Qiu, Y., Feng, J., Shimooka, T., Peng, Y., Xie, Y., Zhu, G., Lu, L., Bao, C., & Ouyang, M. (2024). Temperature‐Inert Interface Enables Safe and Practical Energy‐Dense LiNi 0.91 Co 0.07 Mn 0.02 O 2 Pouch Cells. Advanced Energy Materials, 14(40). https://doi.org/10.1002/aenm.202402638

Vancouver

Hou J, Shi Q, Feng X, Terada J, Wang L, Zhao L, et al. Temperature‐Inert Interface Enables Safe and Practical Energy‐Dense LiNi 0.91 Co 0.07 Mn 0.02 O 2 Pouch Cells. Advanced Energy Materials. 2024;14(40). doi:10.1002/aenm.202402638

BibTeX
@article{Hou2024,
  author = {Hou, Junxian and Shi, Qinyu and Feng, Xuning and Terada, Junpei and Wang, Li and Zhao, Liqi and Cao, Daihua and Yamazaki, Shigeaki and Xu, Chengshan and Qiu, Yue and Feng, Jing and Shimooka, Toshiharu and Peng, Yong and Xie, Yingchen and Zhu, Gaolong and Lu, Languang and Bao, Cheng and Ouyang, Minggao},
  title = {Temperature‐Inert Interface Enables Safe and Practical Energy‐Dense LiNi 0.91 Co 0.07 Mn 0.02 O 2 Pouch Cells},
  journal = {Advanced Energy Materials},
  year = {2024},
  volume = {14},
  number = {40},
  doi = {10.1002/aenm.202402638}
}
Kostenlos starten →