EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Formation‐Stage Interfacial Regulation of δ‐MnO 2 Enables Stable and Reversible Aqueous Zn‐Ion Storage

Fanghua Liang, Ling Wang, Junpeng Xiong iD, Chunqing Niu, Atsuya Kawai, Wei Zhang, Chunhong Zhu iD, Azeem Ullah iD, Mayakrishnan Gopiraman iD, Mingzheng Ge iD, Ick Soo Kim iD

Advanced Science · 04.11.2026

DOI: 10.1002/advs.78465 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Advanced Science, online erschienen am 04.11.2026. Verfasst von Fanghua Liang und 10 weiteren Autor:innen. Beteiligte Einrichtung: Nano Fusion Technology Research Lab, Institute For Fiber Engineering and Science (IFES), Research Cluster for Social Implementation, Shinshu Universi…. Die Arbeit nennt 70 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: New Energy and Industrial Technology Development Organization, JSPS KAKENHI.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Layered δ‐MnO 2 is a promising cathode for aqueous zinc‐ion batteries, yet its practical application remains hindered by the coupled challenges of sluggish Zn 2+ storage kinetics and persistent Mn dissolution. Here, we develop a precursor‐embedded Fe interfacial regulation strategy to modulate the nucleation and growth of δ‐MnO 2 on porous carbon nanofibers (δ‐MnO 2 @Fe‐PCNFs). Rather than being dominated by homogeneous bulk substitution, the introduced Fe is predominantly present as low‐content, highly dispersed surface‐/interface‐associated species established during δ‐MnO 2 formation, where it regulates the local Mn─O environment and consequently modulates nanosheet growth and the accessibility of the reaction interface. The Fe‐regulated δ‐MnO 2 framework exhibits improved kinetic accessibility and suppresses Mn dissolution without altering its intrinsic Mn‐based redox chemistry. Consequently, the δ‐MnO 2 @Fe‐PCNFs electrode delivers an initial capacity of 409.29 mAh g −1 at 0.2 A g −1 and excellent long‑term cycling stability, maintaining a capacity of 243.64 mAh g −1 at 1 A g −1 after 1000 cycles and excellent capacity retention of 81.1% after 3000 cycles at 5 A g −1 . This work highlights formation‐stage interfacial regulation as an effective strategy to couple reaction accessibility with structural durability in Mn‐based aqueous zinc‐ion battery cathodes.

Schlagwörter

Stichwörter der Autor:innen

Fe precursor encodingMn dissolutionMn─O frameworkaqueous zinc‐ion batteryinterfacial electronic regulationδ‐MnO2 nanosheets

Autor:innen und Institutionen

  • Nano Fusion Technology Research Lab, Institute For Fiber Engineering and Science (IFES), Research Cluster for Social Implementation, Shinshu University, Ueda, Nagano, Japan.
  • School of Textile and Clothing, Nantong University, Nantong, People's Republic of China.

ORCID-Profile: Junpeng Xiong, Chunhong Zhu, Azeem Ullah, Mayakrishnan Gopiraman, Mingzheng Ge, Ick Soo Kim

Förderung

  • New Energy and Industrial Technology Development Organization
  • JSPS KAKENHI

Zitieren

APA

Liang, F., Wang, L., Xiong, J., Niu, C., Kawai, A., Zhang, W., Zhu, C., Ullah, A., Gopiraman, M., Ge, M., & Kim, I. S. (2026). Formation‐Stage Interfacial Regulation of δ‐MnO 2 Enables Stable and Reversible Aqueous Zn‐Ion Storage. Advanced Science. https://doi.org/10.1002/advs.78465

Vancouver

Liang F, Wang L, Xiong J, Niu C, Kawai A, Zhang W, et al. Formation‐Stage Interfacial Regulation of δ‐MnO 2 Enables Stable and Reversible Aqueous Zn‐Ion Storage. Advanced Science. 2026. doi:10.1002/advs.78465

BibTeX
@article{Liang2026,
  author = {Liang, Fanghua and Wang, Ling and Xiong, Junpeng and Niu, Chunqing and Kawai, Atsuya and Zhang, Wei and Zhu, Chunhong and Ullah, Azeem and Gopiraman, Mayakrishnan and Ge, Mingzheng and Kim, Ick Soo},
  title = {Formation‐Stage Interfacial Regulation of δ‐MnO 2 Enables Stable and Reversible Aqueous Zn‐Ion Storage},
  journal = {Advanced Science},
  year = {2026},
  doi = {10.1002/advs.78465}
}
Kostenlos starten →