Poisoning Mechanism Map for Metal Hydride Hydrogen Storage Materials
Advanced Science · 2024-11 · 11 (43)
DOI: 10.1002/advs.202408522 ↗Kurz gefasst
Fachartikel in der Zeitschrift Advanced Science, online erschienen am 20.09.2024. Verfasst von Jiapeng Bi und 12 weiteren Autor:innen. Beteiligte Einrichtung: State Key Laboratory of Silicon and Advanced Semiconductor Materials, School of Materials Science and Engineering, Zhejiang University, Hangzhou, Zhe…. Die Arbeit wurde bisher 43-mal zitiert (Crossref) und nennt 43 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: NSAF, National Natural Science Foundation of China, National Key Research and Development Program of China.
Abstract (Originalsprache)
The effective utilization of hydrogen storage materials (HSMs) is hindered by impurity gas poisoning, posing a significant challenge for large‐scale applications. This study elucidates the poisoning mechanisms of various impurities gases (CO, CO 2 , O 2 , Ar, He, CH 4 , N 2 ) on ZrCo, Pd, U and LaNi 5 . Impurities gases are categorized into active and inactive types based on their effecting behaviors and mechanisms on the hydrogenation of HSMs. During the hydrogenation process, active impurities chemically poison the hydrogenation reaction by limiting hydrogen absorption at interface, while inactive impurities physically hinder hydrogenation reaction by impeding hydrogen diffusion in hydrogen‐impurity mixed gas. In situ Scanning Tunneling Microscope clarifies these behaviors, and a novel criterion based on hydrogen spontaneous dissociation energy is introduced to explain and predict impurity–substrate interaction characteristics. The novel findings of this work provide a comprehensive framework for designing long‐lived HSMs with poisoning resistance, guiding the development of more resilient hydrogen storage systems.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- State Key Laboratory of Silicon and Advanced Semiconductor Materials, School of Materials Science and Engineering, Zhejiang University, Hangzhou, Zhejiang, 310058, China.
- College of Materials Science and Engineering, Hohai University, Changzhou, 213200, China.
- Institute of Materials, China Academy of Engineering Physics, Mianyang, Sichuan, 621907, China.
- Key Laboratory of Hydrogen Storage and Transportation Technology of Zhejiang Province, Hangzhou, 310027, China.
ORCID-Profile: Xuezhang Xiao
Förderung
- NSAF
- National Natural Science Foundation of China
- National Key Research and Development Program of China
Zitieren
APA
Bi, J., Zhou, P., Jiang, W., Kou, H., Tang, T., Zhang, Y., Liu, Y., Zhou, Q., Yao, Y., Zhang, Y., Yang, M., Chen, L., & Xiao, X. (2024). Poisoning Mechanism Map for Metal Hydride Hydrogen Storage Materials. Advanced Science, 11(43). https://doi.org/10.1002/advs.202408522
Vancouver
Bi J, Zhou P, Jiang W, Kou H, Tang T, Zhang Y, et al. Poisoning Mechanism Map for Metal Hydride Hydrogen Storage Materials. Advanced Science. 2024;11(43). doi:10.1002/advs.202408522
BibTeX
@article{Bi2024,
author = {Bi, Jiapeng and Zhou, Panpan and Jiang, Wei and Kou, Huaqin and Tang, Tao and Zhang, Yajie and Liu, Yang and Zhou, Qianwen and Yao, Yunxi and Zhang, Yuan and Yang, Mao and Chen, Lixin and Xiao, Xuezhang},
title = {Poisoning Mechanism Map for Metal Hydride Hydrogen Storage Materials},
journal = {Advanced Science},
year = {2024},
volume = {11},
number = {43},
doi = {10.1002/advs.202408522}
}
EUVIMED