Fachartikel in der Zeitschrift Advanced Science, online erschienen am 16.12.2022. Verfasst von Seon Yeong Park und 7 weiteren Autor:innen. Beteiligte Einrichtung: Battery R&D Center, SK On, 325, Expo-ro, Yuseong-gu, Daejeon, 34124, Republic of Korea. Die Arbeit wurde bisher 29-mal zitiert (Crossref) und nennt 75 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Technology Innovation Program, Ministry of Trade, Industry, & Energy.
Abstract (Originalsprache)
Ni‐rich cathodes are the most promising candidates for realizing high‐energy‐density Li‐ion batteries. However, the high‐valence Ni 4+ ions formed in highly delithiated states are prone to reduction to lower valence states, such as Ni 3+ and Ni 2+ , which may cause lattice oxygen loss, cation mixing, and Ni ion dissolution. Further, LiPF 6 , a key salt in commercialized electrolytes, undergoes hydrolysis to produce acidic compounds, which accelerate Ni‐ion dissolution and the interfacial deterioration of the Ni‐rich cathode. Dissolved Ni ions migrate and deposit on the surface of the graphite anode, causing continuous electrolyte decomposition and threatening battery safety by forming Li dendrites on the anode. Herein, 1,2‐bis(diphenylphosphino)ethane (DPPE) chelates Ni ions dissolved from the Ni‐rich cathode using bidentate phosphine moieties and alleviates LiPF 6 hydrolysis via complexation with PF 5 . Further, DPPE reduces the generation of corrosive HF and HPO 2 F 2 substantially compared to the amounts observed using trimethyl phosphite and tris(trimethylsilyl) phosphite, which are HF‐scavenging additives. Li‐ion cells with Ni‐rich cathodes and graphite anodes containing DPPE exhibit remarkable discharge capacity retentions of 83.4%, with high Coulombic efficiencies of >99.99% after 300 cycles at 45 °C. The results of this study will promote the development of electrolyte additives.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- Battery R&D Center, SK On, 325, Expo-ro, Yuseong-gu, Daejeon, 34124, Republic of Korea.
- School of Energy and Chemical Engineering, Ulsan National Institute of Science and Technology (UNIST) 50, UNIST-gil, Ulsan, 44919, Republic of Korea.
- Department of Nuclear Science and Engineering, Massachusetts Institute of Technology, Cambridge, MA, 02139, United States.
- Next Generation Battery Research Center, Korea Electrotechnology Research Institute, 12 Jeongiui-gil, Seongsan-gu, Changwon-si, Gyeongsangnam-do, 51543, Republic of Korea.
- Electro-Functionality Materials Engineering, University of Science and Technology (UST), 217 Gajeong-ro, Yuseong-gu, Daejeon, 34113, Republic of Korea.
- Department of Chemical and Biological Engineering, Korea University, 145 Anam-ro, Seongbuk-gu, Seoul, 02841, Republic of Korea.
ORCID-Profile: Nam-Soon Choi
Förderung
- Technology Innovation Program
- Ministry of Trade, Industry, & Energy
Zitieren
APA
Park, S. Y., Park, S., Lim, H. Y., Yoon, M., Choi, J. H., Kwak, S. K., Hong, S. Y., & Choi, N. S. (2023). Ni‐Ion‐Chelating Strategy for Mitigating the Deterioration of Li‐Ion Batteries with Nickel‐Rich Cathodes. Advanced Science, 10(5). https://doi.org/10.1002/advs.202205918
Vancouver
Park SY, Park S, Lim HY, Yoon M, Choi JH, Kwak SK, et al. Ni‐Ion‐Chelating Strategy for Mitigating the Deterioration of Li‐Ion Batteries with Nickel‐Rich Cathodes. Advanced Science. 2023;10(5). doi:10.1002/advs.202205918
BibTeX
@article{Park2023,
author = {Park, Seon Yeong and Park, Sewon and Lim, Hyeong Yong and Yoon, Moonsu and Choi, Jeong-Hee and Kwak, Sang Kyu and Hong, Sung You and Choi, Nam-Soon},
title = {Ni‐Ion‐Chelating Strategy for Mitigating the Deterioration of Li‐Ion Batteries with Nickel‐Rich Cathodes},
journal = {Advanced Science},
year = {2023},
volume = {10},
number = {5},
doi = {10.1002/advs.202205918}
}
EUVIMED