Asymmetric Sulfonated Nanofibrous Separator for Simultaneously Stabilizing Zn Anodes and Accelerating Cathode Kinetics

Xianbin Zou, Xiaoqing Zhu iD, Qixuan Zhu, Xiuming Li, Long Yu, Aimin Ge iD, Changyong Chase Cao, Guiyin Xu iD, Meifang Zhu iD

Advanced Materials · 2026-11 · 38 (63)

DOI: 10.1002/adma.75145 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Advanced Materials, online erschienen am 25.09.2026. Verfasst von Xianbin Zou und 8 weiteren Autor:innen. Beteiligte Einrichtung: State Key Laboratory of Advanced Fiber Materials, College of Materials Science and Engineering, Donghua University, Shanghai, China. Die Arbeit nennt 63 Literaturangaben. Gefördert von: National Natural Science Foundation of China, Fundamental Research Funds for the Central Universities, Interdisciplinary Frontier Innovation Team Development Special Fund of Donghua University.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

The practical deployment of aqueous zinc metal batteries requires the simultaneous stabilization of the Zn anode interface while maintaining high‐capacity cathode operation. Creating an asymmetric interfacial environment featuring a water‐poor region adjacent to the anode and a water‐rich region adjacent to the cathode suppresses water‐induced dendrite growth and corrosion at the anode while accelerating Zn 2+ /H 2 O insertion kinetics at the cathode. In this study, we report an asymmetric separator consisting of sulfonated poly(phenylene sulfide) (SPPS) nanofibers deposited onto a polypropylene (PP) substrate. Strong ion–dipole interactions between the sulfonate groups and hydrated Zn 2+ promote the desolvation of [Zn(H 2 O) 6 ] 2+ , reduce the number of coordinated water molecules, and consequently suppress dendritic Zn deposition. Meanwhile, water molecules enriched within the nanofibrous layer act as interfacial lubricants, facilitating Zn 2+ intercalation/deintercalation and thereby accelerating cathode reaction kinetics while improving discharge capacity. Zn||Zn cells equipped with the asymmetric separator exhibit stable cycling for 6850 h at 1 mA cm −2 , while Zn||Zn 0.25 V 2 O 5 (ZVO) pouch cells retain 98.2% of their initial capacity after 250 cycles.

Schlagwörter

Stichwörter der Autor:innen

anodecathodechemical engineeringmaterials sciencenanofiberphenylenesulfidesulfonatetaxonomy

Autor:innen und Institutionen

  • State Key Laboratory of Advanced Fiber Materials, College of Materials Science and Engineering, Donghua University, Shanghai, China.
  • Center for Advanced Low-Dimension Materials, College of Materials Science and Engineering, Donghua University, Shanghai, China.
  • Laboratory for Soft Machines & Electronics, Department of Mechanical and Aerospace Engineering, Case Western Reserve University, Cleveland, Ohio, USA.

ORCID-Profile: Xiaoqing Zhu, Aimin Ge, Guiyin Xu, Meifang Zhu

Förderung

  • National Natural Science Foundation of China
  • Fundamental Research Funds for the Central Universities
  • Interdisciplinary Frontier Innovation Team Development Special Fund of Donghua University
  • International Cooperation Fund of the Science and Technology Commission of Shanghai Municipality
  • Shanghai Rising-Star Program

Zitieren

APA

Zou, X., Zhu, X., Zhu, Q., Li, X., Yu, L., Ge, A., Cao, C. C., Xu, G., & Zhu, M. (2026). Asymmetric Sulfonated Nanofibrous Separator for Simultaneously Stabilizing Zn Anodes and Accelerating Cathode Kinetics. Advanced Materials, 38(63). https://doi.org/10.1002/adma.75145

Vancouver

Zou X, Zhu X, Zhu Q, Li X, Yu L, Ge A, et al. Asymmetric Sulfonated Nanofibrous Separator for Simultaneously Stabilizing Zn Anodes and Accelerating Cathode Kinetics. Advanced Materials. 2026;38(63). doi:10.1002/adma.75145

BibTeX
@article{Zou2026,
  author = {Zou, Xianbin and Zhu, Xiaoqing and Zhu, Qixuan and Li, Xiuming and Yu, Long and Ge, Aimin and Cao, Changyong Chase and Xu, Guiyin and Zhu, Meifang},
  title = {Asymmetric Sulfonated Nanofibrous Separator for Simultaneously Stabilizing Zn Anodes and Accelerating Cathode Kinetics},
  journal = {Advanced Materials},
  year = {2026},
  volume = {38},
  number = {63},
  doi = {10.1002/adma.75145}
}