Interfacial Modulation for Anti‐Disproportionation in Zr‐Nb‐Fe‐Ni Based Hydrogen Isotope Storage Alloys Driven by Product Destabilization Strategy
Advanced Materials · 2026-03 · 38 (16)
DOI: 10.1002/adma.202523063 ↗Kurz gefasst
Fachartikel in der Zeitschrift Advanced Materials, online erschienen am 11.02.2026. Verfasst von Zhiyi Yang und 12 weiteren Autor:innen. Beteiligte Einrichtung: State Key Laboratory of Silicon and Advanced Semiconductor Materials; School of Materials Science and Engineering, Zhejiang University, Hangzhou, Chi…. Die Arbeit wurde bisher 2-mal zitiert (Crossref) und nennt 53 Literaturangaben. Gefördert von: National MCF Energy R&D Program, Scientific Research Fund of Zhejiang University.
Abstract (Originalsprache)
Thermal/hydrogen‐induced disproportionation is one of the most fatal obstacles for practical Zr 2 Fe‐based hydrogen isotope storage alloys. Here, an interfacial transport inhibition effect at the disproportionation interface is revealed, in which theoretical screening from a product‐destabilization perspective identifies minor Nb substitution as an effective route to developing a disproportionation‐resistant Zr 1.9 Nb 0.1 Fe 0.7 Ni 0.3 alloy. This composition preserves an ultralow equilibrium hydrogen pressure and accelerated hydrogen absorption kinetics, while simultaneously delivering markedly enhanced resistance to disproportionation and outstanding cycling stability under harsh conditions. By integrating experimental results with thermodynamic and kinetic analyses, this work directs modification studies toward the viewpoint of interfacial transport kinetics for disproportionation. Combined density functional theory analyses and Ab initio molecular dynamics simulations systematically reveal that dispersed substitutional Nb atoms act as interfacial pinning centers at the hydride/disproportionation interfaces, effectively inhibiting detrimental interfacial phase transformation, closely related to weakened interfacial bonding strength, charge transfer, and orbital hybridization. Consequently, disproportionation‐related atomic rearrangement as well as the nucleation and growth of ZrH 2 are kinetically retarded. For the first time, these findings demonstrated that targeted interfacial kinetic engineering constitutes an effective strategy for suppressing disproportionation in Zr 2 Fe‐based hydrogen storage systems.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- State Key Laboratory of Silicon and Advanced Semiconductor Materials; School of Materials Science and Engineering, Zhejiang University, Hangzhou, China.
- Institute of Materials, China Academy of Engineering Physics, Mianyang, China.
- School of Advanced Energy, Sun Yat-Sen University, Shenzhen, China.
- Institute of Wenzhou, Zhejiang University, Wenzhou, China.
- Key Laboratory of Hydrogen Storage and Transportation Technology of Zhejiang Province; Hydrogen Energy Institute, Zhejiang University, Hangzhou, China.
ORCID-Profile: Lixin Chen
Förderung
- National MCF Energy R&D Program
- Scientific Research Fund of Zhejiang University
Zitieren
APA
Yang, Z., Jia, Y., Liu, Y., Huang, J., Chu, F., Shu, L., He, J., Feng, X., Shi, Y., Luo, W., Xiao, X., Fan, X., & Chen, L. (2026). Interfacial Modulation for Anti‐Disproportionation in Zr‐Nb‐Fe‐Ni Based Hydrogen Isotope Storage Alloys Driven by Product Destabilization Strategy. Advanced Materials, 38(16). https://doi.org/10.1002/adma.202523063
Vancouver
Yang Z, Jia Y, Liu Y, Huang J, Chu F, Shu L, et al. Interfacial Modulation for Anti‐Disproportionation in Zr‐Nb‐Fe‐Ni Based Hydrogen Isotope Storage Alloys Driven by Product Destabilization Strategy. Advanced Materials. 2026;38(16). doi:10.1002/adma.202523063
BibTeX
@article{Yang2026,
author = {Yang, Zhiyi and Jia, Yuxiao and Liu, Yang and Huang, Jiajie and Chu, Fei and Shu, Liyang and He, Jiahuan and Feng, Xingwen and Shi, Yan and Luo, Wenhua and Xiao, Xuezhang and Fan, Xiulin and Chen, Lixin},
title = {Interfacial Modulation for Anti‐Disproportionation in Zr‐Nb‐Fe‐Ni Based Hydrogen Isotope Storage Alloys Driven by Product Destabilization Strategy},
journal = {Advanced Materials},
year = {2026},
volume = {38},
number = {16},
doi = {10.1002/adma.202523063}
}
EUVIMED