Fachartikel in der Zeitschrift Advanced Materials, online erschienen am 25.10.2025. Verfasst von Yun Liu und 13 weiteren Autor:innen. Beteiligte Einrichtung: School of Materials Science and Engineering, Beijing Key Laboratory of Environmental Science and Engineering, Beijing Institute of Technology, Beijin…. Die Arbeit wurde bisher 61-mal zitiert (Crossref) und nennt 47 Literaturangaben. Gefördert von: National Key R&D Program of China, High-Level Talent Introduction Project of Yibin, Postdoctoral Fellowship Program of CPSF.
Abstract (Originalsprache)
Single‐crystal nickel‐rich LiNi x Co y Mn 1‐x‐y O 2 (SCNCM, x ≥ 0.9) has emerged as a promising cathode material for lithium‐ion batteries, owing to high energy density and robust crystal structure. However, severe phase transitions contribute to performance degradation and mechanical instability during long‐term cycling. To address these challenges, a uniform liquid film strategy is proposed for the in situ construction of a 3D Li 1.3 Al 0.1 Sc 0.2 Ti 1.7 (PO 4 ) 3 (LASTP) conductive network at (003) plane of SCNCM interface. This network establishes an interface bonding—via Sc─O and Al─O bonds—between SCNCM particles and LASTP. The LASTP framework facilitates rapid lithium‐ion conduction, while the Sc─O and Al─O bonds stabilize oxygen vacancies, thereby suppressing oxygen evolution and enhancing interfacial structural integrity. This mitigates the irreversible phase transition (especially O3 to O1) and lattice deformation. The feasibility and effectiveness of this 3D network approach are substantiated through a combination of experimental investigations, DFT calculations, BEVL network analysis, and COMSOL simulations. As expected, the pouch‐type full battery can achieve a satisfactory capacity retention of 83.7% after 1900 cycles (85.8% at 2.8–4.25 V after 1200 cycles). Furthermore, it provides an extraordinary capacity retention of 79.1% with 161.9 mAh g −1 after 800 cycles in 2.8–4.4 V at 50 °C.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- School of Materials Science and Engineering, Beijing Key Laboratory of Environmental Science and Engineering, Beijing Institute of Technology, Beijing, 100081, P. R. China.
- Chongqing Innovation Center, Beijing Institute of Technology, Beijing, 100081, P. R. China.
- China Electric Power Research Institute, Beijing, 100192, P. R. China.
ORCID-Profile: Lai Chen
Förderung
- National Key R&D Program of China
- High-Level Talent Introduction Project of Yibin
- Postdoctoral Fellowship Program of CPSF
- China Postdoctoral Science Foundation
- National Natural Science Foundation of China
- National Key Research and Development Program of China
Zitieren
APA
Liu, Y., Dong, J., Guan, Y., Wang, X., Chen, Z., Gao, M., Guo, S., Yan, K., Lu, Y., Wang, M., Li, N., Su, Y., Wu, F., & Chen, L. (2026). In Situ 3D Conductive Networks and Interfacial Bonding to Stabilize Oxygen Vacancies for Single‐Crystal Ni‐Rich Cathodes. Advanced Materials, 38(5). https://doi.org/10.1002/adma.202515106
Vancouver
Liu Y, Dong J, Guan Y, Wang X, Chen Z, Gao M, et al. In Situ 3D Conductive Networks and Interfacial Bonding to Stabilize Oxygen Vacancies for Single‐Crystal Ni‐Rich Cathodes. Advanced Materials. 2026;38(5). doi:10.1002/adma.202515106
BibTeX
@article{Liu2026,
author = {Liu, Yun and Dong, Jinyang and Guan, Yibiao and Wang, Xuanzhi and Chen, Zhili and Gao, Mengyuan and Guo, Shiyuan and Yan, Kang and Lu, Yun and Wang, Meng and Li, Ning and Su, Yuefeng and Wu, Feng and Chen, Lai},
title = {In Situ 3D Conductive Networks and Interfacial Bonding to Stabilize Oxygen Vacancies for Single‐Crystal Ni‐Rich Cathodes},
journal = {Advanced Materials},
year = {2026},
volume = {38},
number = {5},
doi = {10.1002/adma.202515106}
}
EUVIMED